Polymer Property : Izod Impact, Notched = 8.30 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 4.43 J/cm

@Temperature -30.0 °C
8.30 ft-lb/in

@Temperature -22.0 °F
ASTM D256
LG Chemical LUPOY HF-5000 High Flow PC/ABS Alloy, Unreinforced
Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive..
Izod Impact, Notched 4.43 J/cm

@Temperature 23.0 °C
8.30 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Eastman Tenite 307A4000015 Propionate Clear, Trsp
Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi..
Izod Impact, Notched 4.43 J/cm

@Temperature 23.0 °C
8.30 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Eastman Tenite 380A4000015 Cellulose Acetate Propionate, Clear, Trsp
Applications:OphthalmicsProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel..