Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 3.82 J/cm @Thickness 6.35 mm |
7.16 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Infino® HI-1001BN PC/ABS, Unreinforced PC/ABS that is used for the housing of mobile phone, wheel cap, rice cooker, electric iron etc., refrigerator door handle, panel etc.Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 3.82 J/cm @Thickness 6.35 mm |
7.16 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Starex® SP-0170 ABS, Unreinforced Extrusion Grade Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 3.82 J/cm @Thickness 6.35 mm |
7.16 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Starex® SP-0170 ABS, Unreinforced Extrusion Grade Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 3.82 J/cm @Thickness 6.35 mm |
7.16 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Infino® HI-1001BN PC/ABS, Unreinforced PC/ABS that is used for the housing of mobile phone, wheel cap, rice cooker, electric iron etc., refrigerator door handle, panel etc.Information provided by Samsung Cheil Industries. |