Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 3.74 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
7.01 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM-D256 |
Ineos ABS Lustran® 750 ABS, Molding Grade Lustran® 750 resin is a black, virgin injection molding grade of ABS (Acrylonitrile Butadiene Styrene). It is designed for molded drain, waste, and vent (DWV) fittings. Lustran® 750 (901802 bl.. |
|||
Izod Impact, Notched | 3.74 J/cm @Thickness 3.17 mm, Temperature -30.0 °C |
7.01 ft-lb/in @Thickness 0.125 in, Temperature -22.0 °F |
ASTM D256 |
Diamond Polymers DIAMALOY PC 1812 Impact Modified Polycarbonate Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |