Polymer Property : Izod Impact, Notched = 6.74 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 3.60 J/cm

@Temperature 23.0 °C
6.74 ft-lb/in

@Temperature 73.4 °F
ISO 75-2/B
Styron MAGNUMâ„¢ 1250 BG Acrylonitrile Butadiene Styrene (ABS) Resin
Overview: High Impact, High Heat, Blow Molding ABSInformation provided by Styron
Izod Impact, Notched 3.60 J/cm

@Thickness 6.35 mm
6.74 ft-lb/in

@Thickness 0.250 in
ASTM D256
Chi Mei Polylac® PA-747R ABS - Extrusion
Attach case and refrigerator