Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 5.71 J/cm @Temperature 23.0 °C |
10.7 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Noble Polymers Regis™ 235107 Thermoplastic Olefin (TPO) Regis is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. We have created Regis for use in bumpers and bumper fascias, air dams, exterior panels, materi.. |
|||
Izod Impact, Notched | 5.71 J/cm @Thickness 3.17 mm, Temperature -28.9 °C |
10.7 ft-lb/in @Thickness 0.125 in, Temperature -20.0 °F |
ASTM D-256 |
Axiall Suprel® 9422 Rigid PVC, Molding Georgia Gulf Suprel® 9422 Alloy is engineered for injection molding applications that require outstanding impact resistance or toughness, particularly at low temperatures. This alloy complies with.. |