Polymer Property : Izod Impact, Notched = 5.40 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 2.88 J/cm

@Temperature 23.0 °C
5.40 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics Prevex VFAX PPE+PS
High impact strength. 180F (82C) HDT. Improved productivity/reliability.This data was supplied by SABIC-IP for the Americas region.
Izod Impact, Notched 2.88 J/cm

@Temperature 23.0 °C
5.40 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Eastman Tenite 383A2R30010 Cellulose Acetate Propionate, Natural, Trsp
Applications:Oral HygienePlastics for hygiene feminine productsRecreationalToothbrushesProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughne..
Izod Impact, Notched 2.88 J/cm

@Thickness 3.17 mm
5.40 ft-lb/in

@Thickness 0.125 in
ASTM D256
Chi Mei Polylac® PA-717C ABS
Medium impact
Izod Impact, Notched 2.88 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
5.40 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
ASTM D-256
Axiall 8607 Rigid PVC, Extrusion
Georgia Gulf 8607 is a special purpose pelletized compound formulated for high impact, rigid extrusion profiles.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.