Mechanical Properties Metric English Comments
Izod Impact, Notched 2.50 J/cm

@Temperature -30.0 °C
4.68 ft-lb/in

@Temperature -22.0 °F
ASTM D 256
SABIC Innovative Plastics Cycoloy® CX1440 PC+ABS (Europe-Africa-Middle East)
CYCOLOY CX1440 is a general purpose PC+ABS blend specially developped for thin wall applications requiring weld line strength and high flow with a good balance of propertiesThis data was supplied by..
Izod Impact, Notched 2.50 J/cm

@Temperature -30.0 °C
4.68 ft-lb/in

@Temperature -22.0 °F
ASTM D 256
SABIC Innovative Plastics Cycoloy® CX5430 PC+ABS (Europe-Africa-Middle East)
Cycoloy* resin CX5430 is a general purpose PC/ABS blend developed for thin wall applications requiring weld line strength, high flow and impact together with a good balance of other properties.This ..
Izod Impact, Notched 2.50 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
4.68 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
Mapal Plastics Maplon CFA-HK Polypropylene Sheet
Applications: For use with electrical insulation products. For use when flame retardant and static dissipative properties are required.
Izod Impact, Notched >= 2.50 J/cm

@Thickness 3.20 mm,
Temperature -30.0 °C
>= 4.68 ft-lb/in

@Thickness 0.126 in,
Temperature -22.0 °F
ASTM D256
Kingfa JH950-402 Flame Retardant PC/ABS Alloy
Features:UL V-0 @ 3.2mmExcellent balance propertiesHigh heat resistanceGood normal/low temperature impact strengthGood surfaceApplications:Small household appliance cabinetControllerSocketShell of a..
Izod Impact, Notched 2.50 J/cm

@Temperature -40.0 °C
4.68 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Lavergne VYPET VNT 1021 Polyester-PC Alloy
The Vypet 1021 Black is a medium viscosity Polyester and PC alloy, has an excellent balance of stiffness and impact resistance.Features: Excellent Processability; Good Impact Resistance; Good Chemic..
Izod Impact, Notched 2.50 J/cm

@Temperature 23.0 °C
4.68 ft-lb/in

@Temperature 73.4 °F
Practical Use (Water Absorption 2.0%); ASTM-D256
Toyobo GLAMIDE® T-403 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Izod Impact, Notched 2.50 J/cm

@Temperature 23.0 °C
4.68 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
Cossa Polimeri ESTADIENE 2525 AS Acrylonitrile Butadiene Styrene
ABS with high impact resistanceGood melt flow rate, with antistatic, excellent processabilityInformation provided by Cossa Polimeri S.r.l.
Izod Impact, Notched >= 2.50 J/cm

@Thickness 3.20 mm,
Temperature 0.000 °C
>= 4.68 ft-lb/in

@Thickness 0.126 in,
Temperature 32.0 °F
ASTM D256, ISO 180/4a
EPICHEM Epicarb PC Polycarbonate
Characteristics: high fluidity, good impact