Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 2.45 J/cm @Temperature -10.0 °C |
4.59 ft-lb/in @Temperature 14.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Geloy XTPM307 ASA+PC (Europe-Africa-Middle East) XTPM307 is a high heat resistant PC/ASA with improved processing stability over HRA150. Typical values measured on natural material.This data was supplied by SABIC-IP for the Europe-Africa-Middle Ea.. |
|||
Izod Impact, Notched | 2.45 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
4.59 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical AF312 ABS, Flame Retardant Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 79-94-7 and 1309-64-4Information provided by LG Chemical.. |
|||
Izod Impact, Notched | 2.45 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
4.59 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical AF312B ABS, Flame Retardant Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 79-94-7 and 1309-64-4Information provided by LG Chemical.. |
|||
Izod Impact, Notched | 2.45 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
4.59 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical AF312C ABS, Flame Retardant Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 79-94-7 and 1309-64-4Information provided by LG Chemical.. |
|||
Izod Impact, Notched | 2.45 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
4.59 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical AF312C ABS, Flame Retardant Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 79-94-7 and 1309-64-4Information provided by LG Chemical.. |
|||
Izod Impact, Notched | 2.45 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
4.59 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical AF360S ABS, TBBA-free Flame Retardant, Low Flow Feature: Injection Molding, TBBA-free Flame Retardant, Low FlowApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 84852-53-9 and 1309-64-4Information .. |
|||
Izod Impact, Notched | 2.45 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
4.59 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical ER460 ABS, Medium Heat Resistance, High Flowability Feature: Injection Molding, Medium Heat Resistance, High FlowabilityApplication: Automobile, Motor Cycle, Electric & Electronic GoodsCAS No. 9003-56-9Information provided by LG Chemical |
|||
Izod Impact, Notched | 2.45 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
4.59 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical ER460 ABS, Medium Heat Resistance, High Flowability Feature: Injection Molding, Medium Heat Resistance, High FlowabilityApplication: Automobile, Motor Cycle, Electric & Electronic GoodsCAS No. 9003-56-9Information provided by LG Chemical |
|||
Izod Impact, Notched | 2.45 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
4.59 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical HF380G ABS, High Flow Feature: Injection Molding, High FlowApplication: Electric & Electronic Products)CAS No. 9003-56-9Information provided by LG Chemical |
|||
Izod Impact, Notched | 2.45 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
4.59 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical HF380U ABS, High Flow Feature: Injection Molding, High Flow, Good WeatherabilityApplication: Electric & Electronic Products, Miscellaneous Goods)CAS No. 9003-56-9Information provided by LG Chemical |
|||
Izod Impact, Notched | 2.45 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
4.59 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical HG173 ABS, High Surface Gloss Feature: Injection Molding, High Surface GlossApplication: Electric & Electronic Products)CAS No. 9003-56-9Information provided by LG Chemical |
|||
Izod Impact, Notched | 2.45 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
4.59 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LG703W ABS, Low Gloss, Heat Resistance Feature: Injection Molding, Low Gloss, Heat ResistanceApplication: Automobiles Interior Housing (Column Cover, Filllar Etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information provided.. |
|||
Izod Impact, Notched | 2.45 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
4.59 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical ER461 ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Automotives Interior & Exterior Housing (Garnish etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information provided by LG Chemica.. |
|||
Izod Impact, Notched | 2.45 J/cm @Thickness 3.17 mm |
4.59 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® SR-0315 V ABS, Unreinforced Heat Resistant Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 2.45 J/cm @Thickness 3.17 mm |
4.59 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® VE-0860SE ABS, Unreinforced FR Flame-retardant ABS material that can be used in the exterior of adaptors, chargers etc.Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 2.45 J/cm @Thickness 3.17 mm |
4.59 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® GW-3130 PC, 10% Glass Filled Recycled Eco-friendly Post-Consumer recycled content.Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 2.45 J/cm @Thickness 6.35 mm, Temperature -30.0 °C |
4.59 ft-lb/in @Thickness 0.250 in, Temperature -22.0 °F |
ASTM D256 |
Samsung Cheil Industries Infino® WP-1041G PC/ABS, Unreinforced Metal Plating Grade Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 2.45 J/cm @Thickness 3.17 mm |
4.59 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® SR-0315 V ABS, Unreinforced Heat Resistant Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 2.45 J/cm @Thickness 3.17 mm |
4.59 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® VE-0860SE ABS, Unreinforced FR Flame-retardant ABS material that can be used in the exterior of adaptors, chargers etc.Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 2.45 J/cm @Temperature 23.0 °C |
4.59 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Verton NV0081EV_GY7E149 PC+ABS Preliminary data for 40% long fiber single pellet non-halogen FR color filled PC/ABSThis data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 2.45 J/cm @Temperature -20.0 °C |
4.59 ft-lb/in @Temperature -4.00 °F |
ASTM D256 |
SCG Chemicals EL-Leneâ„¢ H1000PC High Density Polyethylene Pipe Resin Key Characteristics: Good processing, high thermal stability, low sagging, good balance of MRS, SCG, and RCPRecommended Applications: Water pressure and gas pipesCertification: Certified by EXOVA.. |
|||
Izod Impact, Notched | 2.45 J/cm @Thickness 6.40 mm |
4.59 ft-lb/in @Thickness 0.252 in |
ASTM D256 |
Bhansali Engineering Abstron HI40H ABS Injection Molding Grade Automotive applications -Medium Impact, Super High Rigidity, PaintableInformation provided by Bhansali |
|||
Izod Impact, Notched | 2.45 J/cm @Thickness 3.20 mm |
4.59 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Bhansali Engineering Abstron HR60N ABS Heat Resistant High ImpactInformation provided by Bhansali |
|||
Izod Impact, Notched | 2.45 J/cm @Thickness 6.40 mm |
4.59 ft-lb/in @Thickness 0.252 in |
ASTM D256 |
Bhansali Engineering Abstron SE32 FR IS15061 Flame Retardant ABS Flame Retardant- IS 15061 conformedInformation provided by Bhansali |
|||
Izod Impact, Notched | 2.45 J/cm @Thickness 3.20 mm |
4.59 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Bhansali Engineering Abstron HR60N ABS Heat Resistant High ImpactInformation provided by Bhansali |
|||
Izod Impact, Notched | 2.45 J/cm @Thickness 6.40 mm |
4.59 ft-lb/in @Thickness 0.252 in |
ASTM D256 |
Bhansali Engineering Abstron SE32 FR IS15061 Flame Retardant ABS Flame Retardant- IS 15061 conformedInformation provided by Bhansali |
|||
Izod Impact, Notched | 2.45 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
4.59 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
Asahi Kasei Xyron® X9108 Modified Polyphenylene Ether High-Heat ResistantInformation provided by Asahi Kasei |
|||
Izod Impact, Notched | 2.45 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
4.59 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LI923 Extrusion ASA Description: Good Weatherability, High RigidityApplication: Communication Instrument Cover, Cable Connecting Cover, Door PanelCAS: 26299-47-8Information provided by LG Chemical |
|||
Izod Impact, Notched | 2.45 J/cm @Thickness 6.35 mm, Temperature -30.0 °C |
4.59 ft-lb/in @Thickness 0.250 in, Temperature -22.0 °F |
ASTM D256 |
Samsung Cheil Industries Infino® WP-1041G PC/ABS, Unreinforced Metal Plating Grade Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 2.45 - 2.75 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
4.59 - 5.14 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D256 |
Samyang Triel® 5550 Thermoplastics Polyetherester Elastomer, General Extrusion Excellent mechanical characteristics, elasticity, thermal resistance and chemical resistance.5550 is an extrusion grade.Information provided by Samyang. |