Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 4.16 J/cm @Temperature 23.0 °C |
7.79 ft-lb/in @Temperature 73.4 °F |
3.2 mm (0.125 in) notch |
Kraton® D1102 + PP blend (25/75) Unmodified polypropylene has high rigidity and good heat resistance, but poor impact resistance, especially at low temperatures. Blending KRATON D and G polymers with PP significantly improves the .. |
|||
Izod Impact, Notched | 4.16 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
7.80 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D256 |
Techmer ES Plastiblend® ABS 8014 Availability: North AmericaForms: PelletsProcessing Method: ExtrusionInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 4.16 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
7.80 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D256 |
Techmer ES Plastiblend® ABS 8002 Availability: North AmericaForms: PelletsFeatures: High Heat ResistanceProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 4.16 J/cm @Temperature 23.0 °C |
7.79 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Eastman Tenite 350A0096914 Propionate Natural Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi.. |
|||
Izod Impact, Notched | 4.16 J/cm @Temperature 23.0 °C |
7.79 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Eastman Tenite 360A4000012 Propionate Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi.. |
|||
Izod Impact, Notched | 4.16 J/cm @Temperature 23.0 °C |
7.79 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Eastman Tenite 360E3V45512 Propionate Water Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi.. |
|||
Izod Impact, Notched | 4.16 J/cm @Temperature 23.0 °C |
7.79 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Eastman Tenite 360E461312 Propionate Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi.. |
|||
Izod Impact, Notched | 4.16 J/cm @Temperature 23.0 °C |
7.79 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Eastman Tenite 371A4000012 Cellulose Acetate Propionate, Clear, Trsp Applications:OphthalmicsOral HygienePen/stationary suppliesToothbrushesProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, st.. |