Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 3.73 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
6.98 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical PT270 ABS Feature: Injection Molding, Good PaintabilityApplication: Exterior Part of Automobile and Motor cycleCAS No. 9003-56-9Information provided by LG Chemical |
|||
Izod Impact, Notched | 3.73 J/cm @Thickness 6.35 mm |
6.98 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Starex® SD-0170 F ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 3.73 J/cm @Thickness 6.35 mm |
6.98 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Starex® SD-0170 F ABS, Unreinforced Information provided by Samsung Cheil Industries. |