Polymer Property : Izod Impact, Notched = 2.80 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 1.49 J/cm

@Thickness 3.17 mm,
Temperature 0.000 °C
2.80 ft-lb/in

@Thickness 0.125 in,
Temperature 32.0 °F
ASTM D256
Techmer ES Plastiblend® ABS E
Availability: North AmericaForms: PelletsFeatures: High ViscosityProcessing Method: Blow Molding and ExtrusionInformation provided by TP Composites, Inc.
Izod Impact, Notched 1.49 J/cm

@Thickness 3.17 mm
2.80 ft-lb/in

@Thickness 0.125 in
ASTM D256
Samsung Cheil Industries Starex® SR-0340M High Heat Grade ABS
Information provided by Polymer Technology and Services, LLC (PTS).
Izod Impact, Notched 1.49 J/cm

@Thickness 3.17 mm
2.80 ft-lb/in

@Thickness 0.125 in
ASTM D256
Samsung Cheil Industries Starex® SR-0340M High Heat Grade ABS
Information provided by Polymer Technology and Services, LLC (PTS).
Izod Impact, Notched 1.49 J/cm

@Thickness 3.17 mm,
Temperature 22.8 °C
2.80 ft-lb/in

@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D256
Techmer ES Electrablend® PA6/6 03002 A MB Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement/Unspecified Filler/Reinfor.Additive: Lubricant, Impact Modifier and Heat StabilizerFeatures: Lubricated, Elec..
Izod Impact, Notched 1.49 J/cm

@Thickness 3.17 mm,
Temperature 0.000 °C
2.80 ft-lb/in

@Thickness 0.125 in,
Temperature 32.0 °F
ASTM D256
Techmer ES Plastiblend® ABS HH BK MB
Availability: North AmericaForms: PelletsFeatures: High Gloss and High Heat ResistanceAppearance: BlackProcessing Method: Injection MoldingInformation provided by TP Composites, Inc.
Izod Impact, Notched 1.49 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
2.80 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
ASTM D256
Chi Mei Kibilac® PW-978B ASA, High Heat
Acrylonitrile/Styrene/AcrylateInformation provided by Calsak Corporation
Izod Impact, Notched 1.49 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
2.80 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
ASTM D256
Chi Mei Kibilac® PW-978D ASA, High Heat  (discontinued **)
Acrylonitrile/Styrene/AcrylateInformation provided by Calsak Corporation
Izod Impact, Notched 1.49 J/cm

@Thickness 6.35 mm
2.80 ft-lb/in

@Thickness 0.250 in
ASTM D256
PlastxWorld CEVIAN®-V T150 ABS
Medium impact transparent ABS.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc.