Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.44 J/cm @Temperature -30.0 °C |
2.70 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® FXD103 PC FXD103 is a Light Diffusion effect, part of the VisualFX family. These effects have been developed to meet increasing Aesthetic demands in the Marketplace.This data was supplied by SABIC-IP for the .. |
|||
Izod Impact, Notched | 1.44 J/cm @Temperature -30.0 °C |
2.70 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® FXD103 PC (Asia Pacific) FXD103 is a Light Diffusion effect, part of the VisualFX family. These effects have been developed to meet increasing Aesthetic demands in the Marketplace.This data was supplied by SABIC-IP for the .. |
|||
Izod Impact, Notched | 1.44 J/cm @Temperature -30.0 °C |
2.70 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® FXD103 PC (Europe-Africa-Middle East) FXD103 is a Light Diffusion effect, part of the VisualFX family. These effects have been developed to meet increasing Aesthetic demands in the Marketplace.This data was supplied by SABIC-IP for the .. |
|||
Izod Impact, Notched | 1.44 J/cm @Thickness 6.35 mm |
2.70 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
PTS Trilac® FR3800 Flame Retardant ABS Resin, RoHS Compliant Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Izod Impact, Notched | 1.44 J/cm @Thickness 6.35 mm |
2.70 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
PTS Trilac® FR3800-V Flame Retardant ABS Resin, RoHS Compliant Contains UV absorber.Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Izod Impact, Notched | 1.44 J/cm @Temperature -30.0 °C |
2.70 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® HPH4504 PPC High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, steam, gamma and e-beam steril.. |
|||
Izod Impact, Notched | 1.44 J/cm @Temperature -30.0 °C |
2.70 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® HPH4504H PPC (Europe-Africa-Middle East) High heat specialty polycarbonate with enhanced autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, .. |
|||
Izod Impact, Notched | 1.44 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
2.70 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Edgetek® XT XT-115GF-AX01-HF PC+PBT with Glass Fiber Reinforcement
(discontinued **) EDGETEK™ XT High Performance Polymers are polycarbonate and polyester alloys that combine strength, durability and chemical resistance. The Edgetek XT product family includes a complete line of gen.. |
|||
Izod Impact, Notched | 1.44 J/cm @Temperature -30.0 °C |
2.70 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® ML5472 PC Gamma sterilization resistant. High heat (PPC). Available in natural color only. Internal mold release.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 1.44 J/cm @Temperature -20.0 °C |
2.70 ft-lb/in @Temperature -4.00 °F |
1/8'' notched bar; ASTM D256 |
Ineos N20L-00 Polypropylene Impact Copolymer This is a nucleated polypropylene impact copolymer formulated with a slip agent for improved mold release, and has an optimum balance of stiffness and impact resistance for injection molding applica.. |
|||
Izod Impact, Notched | 1.44 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
2.70 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D256 |
Techmer ES Plastiblend® PC/PBT IM 1702 BK Availability: North AmericaForms: PelletsAdditive: Impact ModifierFeatures: Impact ModifiedAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 1.44 J/cm @Thickness 3.17 mm |
2.70 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Chi Mei Polylac® PA-707 ABS High gloss, high rigid |
|||
Izod Impact, Notched | 1.44 J/cm @Thickness 6.35 mm |
2.70 ft-lb/in @Thickness 0.250 in |
|
Chi Mei Polylac® PA-707 ABS High gloss, high rigid |
|||
Izod Impact, Notched | 1.44 J/cm @Thickness 3.17 mm |
2.70 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Chi Mei Polylac® PA-764 ABS - Flame Retardant F.R. Weather Resistant |
|||
Izod Impact, Notched | 1.44 J/cm @Thickness 6.35 mm |
2.70 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Chi Mei Polylac® PA-777D ABS - High Heat Super High Heat |
|||
Izod Impact, Notched | 1.44 J/cm @Thickness 6.35 mm |
2.70 ft-lb/in @Thickness 0.250 in |
ASTM D-256 |
Axiall 7751 Rigid PVC, Extrusion Georgia Gulf 7751 is a vertical blind profile exterior compound requiring the following properties: Impact Strength & ToughnessColorabilityDimensional StabilityUV Color StabilityEasy Processing in .. |
|||
Izod Impact, Notched | 1.44 J/cm @Temperature -29.0 °C |
2.70 ft-lb/in @Temperature -20.2 °F |
3.2 mm (0.125 in) notch |
Kraton® G1657 + PA-6 blend (16/4/80) Blending KRATON D and G polymers with PA significantly improves the toughness at both room and low temperatures. KRATON polymers are block segments of styrene and rubber monomers (A-B, A-B-A, or [A.. |