Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 2.50 J/cm @Temperature -30.0 °C |
4.68 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycoloy® CX1440 PC+ABS (Europe-Africa-Middle East) CYCOLOY CX1440 is a general purpose PC+ABS blend specially developped for thin wall applications requiring weld line strength and high flow with a good balance of propertiesThis data was supplied by.. |
|||
Izod Impact, Notched | 2.50 J/cm @Temperature -30.0 °C |
4.68 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycoloy® CX5430 PC+ABS (Europe-Africa-Middle East) Cycoloy* resin CX5430 is a general purpose PC/ABS blend developed for thin wall applications requiring weld line strength, high flow and impact together with a good balance of other properties.This .. |
|||
Izod Impact, Notched | 2.50 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
4.68 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
Mapal Plastics Maplon CFA-HK Polypropylene Sheet Applications: For use with electrical insulation products. For use when flame retardant and static dissipative properties are required. |
|||
Izod Impact, Notched | >= 2.50 J/cm @Thickness 3.20 mm, Temperature -30.0 °C |
>= 4.68 ft-lb/in @Thickness 0.126 in, Temperature -22.0 °F |
ASTM D256 |
Kingfa JH950-402 Flame Retardant PC/ABS Alloy Features:UL V-0 @ 3.2mmExcellent balance propertiesHigh heat resistanceGood normal/low temperature impact strengthGood surfaceApplications:Small household appliance cabinetControllerSocketShell of a.. |
|||
Izod Impact, Notched | 2.50 J/cm @Temperature -40.0 °C |
4.68 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Lavergne VYPET VNT 1021 Polyester-PC Alloy The Vypet 1021 Black is a medium viscosity Polyester and PC alloy, has an excellent balance of stiffness and impact resistance.Features: Excellent Processability; Good Impact Resistance; Good Chemic.. |
|||
Izod Impact, Notched | 2.50 J/cm @Temperature 23.0 °C |
4.68 ft-lb/in @Temperature 73.4 °F |
Practical Use (Water Absorption 2.0%); ASTM-D256 |
Toyobo GLAMIDE® T-403 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Izod Impact, Notched | 2.50 J/cm @Temperature 23.0 °C |
4.68 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
Cossa Polimeri ESTADIENE 2525 AS Acrylonitrile Butadiene Styrene ABS with high impact resistanceGood melt flow rate, with antistatic, excellent processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | >= 2.50 J/cm @Thickness 3.20 mm, Temperature 0.000 °C |
>= 4.68 ft-lb/in @Thickness 0.126 in, Temperature 32.0 °F |
ASTM D256, ISO 180/4a |
EPICHEM Epicarb PC Polycarbonate Characteristics: high fluidity, good impact |