Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.28 J/cm @Temperature -30.0 °C |
2.40 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® 945ASR PC Lexan* 945ASR Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is available in transparent and t.. |
|||
Izod Impact, Notched | 1.28 J/cm @Temperature -30.0 °C |
2.40 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® 945ASR PC (Asia Pacific) Lexan* 945ASR Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is available in transparent and t.. |
|||
Izod Impact, Notched | 1.28 J/cm @Temperature -30.0 °C |
2.40 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® 945ASR PC (Europe-Africa-Middle East) Lexan* 945ASR Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is available in transparent and t.. |
|||
Izod Impact, Notched | 1.28 J/cm @Thickness 3.20 mm, Temperature -30.0 °C |
2.40 ft-lb/in @Thickness 0.126 in, Temperature -22.0 °F |
ASTM-D256 |
Ineos ABS Lustran® 720 ABS, Molding Grade Lustran® ABS 720 resin is a black, virgin injection molding grade of ABS (acrylonitrile butadiene styrene). It is supplied as salt-and-pepper pellets with color concentrate 901802 black. Designed.. |
|||
Izod Impact, Notched | 1.28 J/cm @Temperature 23.0 °C |
2.40 ft-lb/in @Temperature 73.4 °F |
1/8" (3mm) notched bar; ASTM D256 |
Ineos L80Z-00 Impact Copolymer Polypropylene L80Z-000 impact copolymer polypropylene is a high melt flow rate, nucleated and antistatic grade designed for high-speed injection molding applications. This resin meets the requirements of the U.S... |
|||
Izod Impact, Notched | 1.28 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
2.40 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D256 |
Techmer ES Elastoblend® PA6 GF40 IM2 NAT 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightAdditive: Impact ModifierFeatures: Impact ModifiedUL File Number: E157318Processing Meth.. |
|||
Izod Impact, Notched | 1.28 J/cm @Thickness 6.35 mm |
2.40 ft-lb/in @Thickness 0.250 in |
|
TPI Porene® ABS-AN450 Flame Retardant ABS Resin Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Izod Impact, Notched | 1.28 J/cm @Thickness 3.17 mm, Temperature -18.0 °C |
2.40 ft-lb/in @Thickness 0.125 in, Temperature -0.400 °F |
ASTM D256 |
Diamond Polymers Centrex® 601 Profile Extrusion Grade AES Centrex 601 resin is a very high-impact, low-gloss AES (acrylonitrile-ethylene-propylene-styrene) resin with good resistance to weather aging. It has good melt strength for profile extrusion and can.. |
|||
Izod Impact, Notched | 1.28 J/cm @Temperature 23.0 °C |
2.40 ft-lb/in @Temperature 73.4 °F |
DAM; ASTM D256 |
DuPont Performance Polymers Zytel® 77G33HS1L NC010 Nylon 612 Zytel® 77G33HS1L NC010 is a 33% glass fiber reinforced, heat stabilized polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Izod Impact, Notched | 1.28 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
2.40 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D256 |
Techmer ES Plastiblend® ABS/PA 1700 Availability: North AmericaForms: PelletsAppearance: Natural ColorInformation provided by TP Composites, Inc. |