Polymer Property : Izod Impact, Notched = 2.38 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 2.38 J/cm

@Temperature 23.0 °C
4.46 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics LNP Verton NV0061EV_GY7E148 PC+ABS
Preliminary data for 30% long fiber single pellet non-halogen FR color filled PC/ABSThis data was supplied by SABIC-IP for the Americas region.
Izod Impact, Notched 2.38 J/cm

@Thickness 3.17 mm
4.46 ft-lb/in

@Thickness 0.125 in
ASTM D256
Chi Mei Polylac® PA-777B ABS - High Heat
High Heat Impact