Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 2.35 J/cm @Temperature -30.0 °C |
4.40 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
Noble Polymers Regis™ 250107 Thermoplastic Olefin (TPO) Regis is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. We have created Regis for use in bumpers and bumper fascias, air dams, exterior panels, materi.. |
|||
Izod Impact, Notched | 2.35 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
4.41 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical AF312A ABS, Flame Retardant Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 79-94-7 and 1309-64-4Information provided by LG Chemical.. |
|||
Izod Impact, Notched | 2.35 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
4.41 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical HF380NS ABS, High Flow, General Anti-Static Feature: Injection Molding, High Flow, General Anti-StaticApplication: Electric & Electronic Products, Miscellaneous goods)CAS No. 9003-56-9Information provided by LG Chemical |
|||
Izod Impact, Notched | 2.35 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
4.41 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical HF380NS ABS, High Flow, General Anti-Static Feature: Injection Molding, High Flow, General Anti-StaticApplication: Electric & Electronic Products, Miscellaneous goods)CAS No. 9003-56-9Information provided by LG Chemical |
|||
Izod Impact, Notched | 2.35 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
4.41 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical HG173 ABS, High Surface Gloss Feature: Injection Molding, High Surface GlossApplication: Electric & Electronic Products)CAS No. 9003-56-9Information provided by LG Chemical |
|||
Izod Impact, Notched | 2.35 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
4.41 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LG749W ABS, Low Gloss, Heat Resistance Feature: Injection Molding, Low Gloss, Heat ResistanceApplication: Automotive Interior Housing (Glove Cover, Door S/W Housing Etc)CAS No. 25120-20-1, 9003-56-9 and 25747-74-7Information provided by.. |
|||
Izod Impact, Notched | 2.35 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
4.41 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical PI642G ABS, General Purpose, High Modulus Feature: Extrusion Molding, General Purpose, High ModulusApplication: Pipe fittingCAS No. 9003-56-9Information provided by LG Chemical |
|||
Izod Impact, Notched | 2.35 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
4.41 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical XR401B ABS, High Flow, Heat Resistance Feature: Injection Molding, High Flow, Heat ResistanceApplication: Automotives Exterior Housing (Side Mirror Housing, Garnish etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information p.. |
|||
Izod Impact, Notched | 2.35 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
4.40 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D256 |
Techmer ES Elastoblend® PA6 GF34 IM HS 34% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 34% Filler by WeightAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impac.. |
|||
Izod Impact, Notched | 2.35 J/cm @Thickness 3.17 mm, Temperature 0.000 °C |
4.40 ft-lb/in @Thickness 0.125 in, Temperature 32.0 °F |
ASTM D256 |
Techmer ES Plastiblend® ABS 8003 A1 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and Impact ModifierFeatures: Heat Stabilized and Impact ModifiedProcessing Method: Injection MoldingInformation provided by TP Comp.. |
|||
Izod Impact, Notched | 2.35 J/cm @Thickness 3.17 mm |
4.41 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® LX-0987EXS ABS, Unreinforced Metallic-Look Luminous Grade - gives aesthetics of a painted surface without painting. Reduces time, cost, and environmental hazards (such as soilvents).Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 2.35 J/cm @Thickness 6.35 mm |
4.41 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Starex® QU-0191S ABS, Unreinforced Extrusion Grade Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 2.35 J/cm @Thickness 3.17 mm |
4.41 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® LX-0987EXS ABS, Unreinforced Metallic-Look Luminous Grade - gives aesthetics of a painted surface without painting. Reduces time, cost, and environmental hazards (such as soilvents).Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 2.35 J/cm @Thickness 6.35 mm |
4.41 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Starex® QU-0191S ABS, Unreinforced Extrusion Grade Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 2.35 J/cm @Thickness 3.17 mm |
4.41 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® SR-0305 ABS, Unreinforced Heat Resistant Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 2.35 J/cm @Thickness 6.40 mm |
4.41 ft-lb/in @Thickness 0.252 in |
ASTM D256 |
Bhansali Engineering Abstron IM-11 ABS Injection Molding Grade High Impact, High Rigidity, High Fatigue, Low Flow, PaintableInformation provided by Bhansali |
|||
Izod Impact, Notched | 2.35 J/cm @Thickness 6.40 mm |
4.41 ft-lb/in @Thickness 0.252 in |
ASTM D-256 |
Bhansali Engineering Abstron IM-11BM ABS Injection Molding Grade High Impact Strength, Medium Flow, High Fatigue ResistanceInformation provided by Bhansali |
|||
Izod Impact, Notched | 2.35 J/cm @Thickness 6.40 mm |
4.41 ft-lb/in @Thickness 0.252 in |
ASTM D-256 |
Bhansali Engineering Abstron IM-14G ABS Very High Rigidity Injection Molding Grade Very High Rigidity, High Gloss, Medium Impact with excellent other mechanical propertiesInformation provided by Bhansali |
|||
Izod Impact, Notched | 2.35 J/cm @Thickness 3.20 mm |
4.41 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Bhansali Engineering Abstron KU602 ABS Heat Resistant High ImpactInformation provided by Bhansali |
|||
Izod Impact, Notched | 2.35 J/cm @Thickness 3.20 mm |
4.41 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Bhansali Engineering Abstron KU602L ABS Heat Resistant High rigidityInformation provided by Bhansali |
|||
Izod Impact, Notched | 2.35 J/cm @Thickness 3.20 mm |
4.41 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Bhansali Engineering Abstron KU603 ABS Heat Resistant High Impact, High RigidityInformation provided by Bhansali |
|||
Izod Impact, Notched | 2.35 J/cm @Thickness 6.40 mm |
4.41 ft-lb/in @Thickness 0.252 in |
ASTM D-256 |
Bhansali Engineering Abstron IM-11BM ABS Injection Molding Grade High Impact Strength, Medium Flow, High Fatigue ResistanceInformation provided by Bhansali |
|||
Izod Impact, Notched | 2.35 J/cm @Thickness 3.20 mm |
4.41 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Bhansali Engineering Abstron KU602L ABS Heat Resistant High rigidityInformation provided by Bhansali |
|||
Izod Impact, Notched | 2.35 J/cm @Thickness 6.40 mm |
4.41 ft-lb/in @Thickness 0.252 in |
ASTM D256 |
Bhansali Engineering Abstron IM-11 ABS Injection Molding Grade High Impact, High Rigidity, High Fatigue, Low Flow, PaintableInformation provided by Bhansali |
|||
Izod Impact, Notched | 2.35 J/cm @Thickness 3.20 mm |
4.41 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Bhansali Engineering Abstron KU603 ABS Heat Resistant High Impact, High RigidityInformation provided by Bhansali |
|||
Izod Impact, Notched | 2.35 J/cm @Temperature 23.0 °C |
4.41 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
E-Polymers SEPAZ® LB30 PA6 LFT Resin Long Fiber Thermoplastics: SEPAZ LFT products, injection moldable long fiber-reinforced thermoplastics (LFT), are made using a unique pultrusion that thoroughly wets out the glass fibers and deliver.. |
|||
Izod Impact, Notched | 2.35 J/cm @Temperature -30.0 °C |
4.41 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
E-Polymers SEPAZ® LB30 PA6 LFT Resin Long Fiber Thermoplastics: SEPAZ LFT products, injection moldable long fiber-reinforced thermoplastics (LFT), are made using a unique pultrusion that thoroughly wets out the glass fibers and deliver.. |
|||
Izod Impact, Notched | 2.35 J/cm @Thickness 6.40 mm |
4.41 ft-lb/in @Thickness 0.252 in |
ASTM D-256 |
Bhansali Engineering Abstron IM-14G ABS Very High Rigidity Injection Molding Grade Very High Rigidity, High Gloss, Medium Impact with excellent other mechanical propertiesInformation provided by Bhansali |
|||
Izod Impact, Notched | 2.35 J/cm @Thickness 3.20 mm |
4.41 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Bhansali Engineering Abstron KU602 ABS Heat Resistant High ImpactInformation provided by Bhansali |
|||
Izod Impact, Notched | 2.35 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
4.41 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical SG175G ABS, Super Surface Gloss, High Flow Feature: Injection Molding, Super Surface Gloss, High FlowApplication: Electric & Electronic ProductsCAS No. 9003-56-9Information provided by LG Chemical |