Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.25 J/cm @Thickness 3.20 mm, Temperature -20.0 °C |
2.34 ft-lb/in @Thickness 0.126 in, Temperature -4.00 °F |
ISO 180/4A |
Polimeri Europa Sinkral® B 432/E ABS Resin Sinkral B 432/E is a general purpose extrusion grade which exhibits a good balance between rigidity and toughness. Designation: Thermoplastic ISO 2580-ABS 1,EGN,105-04-16-20Applications: Large sheet.. |
|||
Izod Impact, Notched | 1.25 J/cm @Thickness 3.20 mm, Temperature -40.0 °C |
2.34 ft-lb/in @Thickness 0.126 in, Temperature -40.0 °F |
ISO 180/4A |
Polimeri Europa Sinkral® B 532/E ABS Resin Sinkral B 532/E is an extrusion grade, which combines high toughness with good rigidity. Its rheological characteristics and good thermal stability are required for the production of large extruded .. |
|||
Izod Impact, Notched | 1.25 J/cm @Thickness 3.20 mm, Temperature -20.0 °C |
2.34 ft-lb/in @Thickness 0.126 in, Temperature -4.00 °F |
ISO 180/4A |
Polimeri Europa Sinkral® C 442 ABS Resin Sinkral C 442 is a heat resistant injection molding grade offering good flow and impact resistance together with excellent thermal stability during processing. Designation: Thermoplastic ISO 2580-AB.. |
|||
Izod Impact, Notched | 1.25 J/cm @Thickness 3.20 mm, Temperature 0.000 °C |
2.34 ft-lb/in @Thickness 0.126 in, Temperature 32.0 °F |
ISO 180/4A |
Polimeri Europa Sinkral® F 332 ABS Resin Sinkral F 332 is a general purpose injection molding grade which combines excellent thermal stability during processing with a good balance between flow and impact characteristics. Designation: Ther.. |
|||
Izod Impact, Notched | 1.25 J/cm @Temperature -30.0 °C |
2.34 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® 4301 PPC+PC (Asia Pacific) Lexan 4301 is a high heat resistant poly (ester) carbonate resin for injection moldingThis data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 1.25 J/cm @Temperature -30.0 °C |
2.34 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® 4301 PPC+PC (Europe-Africa-Middle East) Lexan 4301 is a high heat resistant poly (ester) carbonate resin for injection moldingThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Notched | 1.25 J/cm @Temperature -30.0 °C |
2.34 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® AD4820 PC LEXAN AD4820 is a high viscosity grade exhibiting low dust attraction with a UV cut-off up to 400 nm and greater optical purity than standard resin.This data was supplied by SABIC-IP for the America.. |
|||
Izod Impact, Notched | 1.25 J/cm @Temperature -30.0 °C |
2.34 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® 4301 PPC+PC Lexan 4301 is a high heat resistant poly (ester) carbonate resin for injection moldingThis data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 1.25 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
2.34 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
Kingfa NH-627 Flame Retardant ABS Features:UL 94 V-2 @ 1.6mmHalogen-free flame retardantHigh flowApplications:OA deviceDigital cameraVidiconInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Izod Impact, Notched | 1.25 J/cm @Temperature 23.0 °C |
2.34 ft-lb/in @Temperature 73.4 °F |
Absolute Drying; ASTM-D256 |
Toyobo GLAMIDE® T-602G30 MXD66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Izod Impact, Notched | 1.25 J/cm @Thickness 3.20 mm, Temperature -30.0 °C |
2.34 ft-lb/in @Thickness 0.126 in, Temperature -22.0 °F |
ASTM D256, ISO 180/4a |
EPICHEM Epiryl B PPO Polyphenylene oxide |
|||
Izod Impact, Notched | 1.25 J/cm @Temperature -20.0 °C |
2.34 ft-lb/in @Temperature -4.00 °F |
ASTM D256 |
Carmel Olefins CAPILENE® TG 50 Polypropylene Impact Copolymer Description: CAPILENE® TG 50 is a heterophasic copolymer designed for injection molding applications requiring optimal impact resistance. This grade combines excellent impact strength, even at lo.. |