Polymer Property : Izod Impact, Notched = 2.29 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 1.22 J/cm

@Temperature -40.0 °C
2.29 ft-lb/in

@Temperature -40.0 °F
Solvay Specialty Polymers Halar® 300 ECTFE Fluoropolymer  (discontinued **)
Data provided by the manufacturer.HALAR® Fluoropolymers have excellent barrier properties, high resistance to a variety of corrosive chemicals and solvents, low flammability, and ease of processing..
Izod Impact, Notched 1.22 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
2.29 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
Kingfa JH710 G10 Flame Retardant & 10% Glass Reinforced PC
Features:Environmental friendly flame retardantUL V-0 @ 1.6mmHigh mechanical strengthGood size stability, good surfaceSuitable for exact moldingApplications:CD-ROM, DVDPrinter, photocopier cabinetSc..
Izod Impact, Notched 1.22 J/cm

@Temperature -30.0 °C
2.29 ft-lb/in

@Temperature -22.0 °F
ASTM D 256
SABIC Innovative Plastics Xenoy® X6125 PBT+PC
Unreinforced, impact modified, thermoplastic alloy (PBT+PC). High impact strength while retaining mechanical and thermal properties.This data was supplied by SABIC-IP for the Americas region.
Izod Impact, Notched 1.22 J/cm

@Thickness 6.35 mm
2.29 ft-lb/in

@Thickness 0.250 in
ASTM D256
Chi Mei Polylac® PA-764 ABS - Flame Retardant
F.R. Weather Resistant
Izod Impact, Notched 1.22 J/cm

@Thickness 3.17 mm
2.29 ft-lb/in

@Thickness 0.125 in
ASTM D256
Chi Mei Polylac® PA-777E ABS - High Heat
Ultra High Heat