Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 2.2549 J/cm @Thickness 3.20 mm |
4.2244 ft-lb/in @Thickness 0.126 in |
ASTM D-256 |
Bhansali Engineering Abstron IM-17 A EP ABS Electro Plating Applications Electroplating & Hot Stamping GradesInformation provided by Bhansali |
|||
Izod Impact, Notched | 2.2549 J/cm @Thickness 3.20 mm |
4.2244 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Bhansali Engineering Abstron IM-21 ABS Very High Rigidity Injection Molding Grade Very High Rigidity, High Gloss, Medium Impact with excellent other mechanical propertiesInformation provided by Bhansali |
|||
Izod Impact, Notched | 2.2549 J/cm @Thickness 3.20 mm |
4.2244 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Bhansali Engineering Abstron IM-21 ABS Very High Rigidity Injection Molding Grade Very High Rigidity, High Gloss, Medium Impact with excellent other mechanical propertiesInformation provided by Bhansali |
|||
Izod Impact, Notched | 2.2549 J/cm @Thickness 3.20 mm |
4.2244 ft-lb/in @Thickness 0.126 in |
ASTM D-256 |
Bhansali Engineering Abstron IM-17 A EP ABS Electro Plating Applications Electroplating & Hot Stamping GradesInformation provided by Bhansali |