Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Notched = 2.25 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 1.20 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
2.25 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Compression Molded, Across Flow; ASTM D256A
PolyOne Geon™ Vinyl Rigid Extrusion 87775 Polyvinyl Chloride, Rigid (PVC, Rigid)
The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne
Izod Impact, Notched 1.20 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
2.25 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
PolyOne Geon™ Vinyl Rigid Molding 87546 Polyvinyl Chloride, Rigid (PVC, Rigid)
Provisional Data SheetInformation provided by PolyOne
Izod Impact, Notched 1.20 J/cm

@Temperature -30.0 °C
2.25 ft-lb/in

@Temperature -22.0 °F
ASTM D 256
SABIC Innovative Plastics Cycoloy® CE1821 PC+ABS (Europe-Africa-Middle East)
High stiffness PC/ABS blend offering high impact, high heat, low CTE, good surface quality and excellent extrusion and thermoforming characteristics.This data was supplied by SABIC-IP for the Europe..
Izod Impact, Notched 1.20 J/cm

@Temperature -30.0 °C
2.25 ft-lb/in

@Temperature -22.0 °F
ASTM D 256
SABIC Innovative Plastics Cycoloy® CX7110 PC+ABS (Europe-Africa-Middle East)
Cycoloy* resin grade CX7110 is an injection moldable PC/ABS blend with non-brominated and non-chlorinated flame retardant systems. Excellent impact/flow balance together with a UL-94 V0 rating at 1...
Izod Impact, Notched 1.20 J/cm

@Temperature 23.0 °C
2.25 ft-lb/in

@Temperature 73.4 °F
ASTM D256
SABIC PP 57MNK10 Polypropylene Impact Copolymer for Injection Molding
Product Description: PP 57MNK10 is a controlled rheology PP grade of medium molecular weight distribution specially developed for producing injection molded articles. This grade has an excellent i..
Izod Impact, Notched 1.20 J/cm

@Thickness 6.35 mm
2.25 ft-lb/in

@Thickness 0.250 in
ASTM D256
LG Chemical SG-910 Alphalac Polystyrene  (Unverified Data**)
High gloss and high impact equivalent to ABS, Excellent mechanical properties compare with general HIPS, Meet requirements for cost and quality, Applications include housing of electric appliances
Izod Impact, Notched 1.20 J/cm

@Temperature 23.0 °C
2.25 ft-lb/in

@Temperature 73.4 °F
ASTM D256A
Micropol Microstat ML21 Linear medium density static dissipative polyethylene
Information provided by Micropol Limited
Izod Impact, Notched 1.20 J/cm

@Temperature -30.0 °C
2.25 ft-lb/in

@Temperature -22.0 °F
ASTM Test
Styrolution Terluran® HI-10 ABS
Terluran HI-10 is an injection molding and extrusion grade of ABS with very high toughness and medium flow.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS.
Izod Impact, Notched 1.20 J/cm

@Temperature 23.0 °C
2.25 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics Noryl NH3060 PPE+HIPS
NH3060 resin is a modified PPE + PS blend with an excellent balance of non-chlorinated non-brominated flame retardance, hydrolytic stability, impact and heat resistance, good flow, and low specific ..
Izod Impact, Notched 1.20 J/cm

@Temperature 23.0 °C
2.25 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics Noryl PX0003 PPE+HIPS
PX0003 resin is a modified PPE+PS blend with an excellent balance of non-chlorinated non-brominated flame retardance, hydrolytic stability, impact and heat resistance, good flow, and low specific gr..
Izod Impact, Notched 1.20 J/cm

@Temperature 23.0 °C
2.25 ft-lb/in

@Temperature 73.4 °F
Absolute Drying; ASTM-D256
Toyobo GLAMIDE® T-402 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Izod Impact, Notched 1.20 J/cm

@Temperature -40.0 °C
2.25 ft-lb/in

@Temperature -40.0 °F
Practical Use (Water Absorption 1.25%); ASTM-D256
Toyobo GLAMIDE® T-663G50 Nylon-66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Izod Impact, Notched 1.20 J/cm

@Temperature 23.0 °C
2.25 ft-lb/in

@Temperature 73.4 °F
Absolute Drying; ASTM-D256
Toyobo GLAMIDE® T-665C30 Nylon-66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Izod Impact, Notched 1.20 J/cm

@Temperature 23.0 °C
2.25 ft-lb/in

@Temperature 73.4 °F
Absolute Drying; ASTM-D256
Toyobo GLAMIDE® TY-502NZ 6T-Nylon
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Izod Impact, Notched 1.20 J/cm

@Temperature 23.0 °C
2.25 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
Cossa Polimeri ESTABLEND 0820 GF Polycarbonate ABS Blend, 10% Glass Filled
Polycarbonate and Acrylonitrile Butadiene Styrene blend with 10% glass fiber reinforcementGood impact resistance, good thermal resistanceInformation provided by Cossa Polimeri S.r.l.
Izod Impact, Notched 1.20 J/cm

@Temperature 23.0 °C
2.25 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
Cossa Polimeri ESTACARB 0820 GF Polycarbonate, 10% Glass Filled
Polycarbonate with 10% glass fiber reinforcementHigh stiffness, good impact resistanceInformation provided by Cossa Polimeri S.r.l.
Izod Impact, Notched 1.20 J/cm

@Temperature 23.0 °C
2.25 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
Cossa Polimeri ESTACARB 1601 OPALE Polycarbonate
Polycarbonate for injection moldingOpal, light diffusiveInformation provided by Cossa Polimeri S.r.l.
Izod Impact, Notched 1.20 J/cm

@Temperature 23.0 °C
2.25 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
Cossa Polimeri ESTADIENE 1030 V0/F Flame Retardant ABS
Acrylonitrile Butadiene StyreneFlame retardant class V0, PBDE free, high melt flow rate, good impact resistance, high gloss, good light resistance, excellent processabilityInformation provided by Co..
Izod Impact, Notched 1.20 J/cm

@Temperature 23.0 °C
2.25 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
Cossa Polimeri ESTADIENE 1218 V0/B Flame Retardant ABS
Acrylonitrile Butadiene StyreneFlame retardant class V0, PBDE free, good impact resistance, excellent processability, good surface appearanceInformation provided by Cossa Polimeri S.r.l.
Izod Impact, Notched 1.20 J/cm

@Temperature 23.0 °C
2.25 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
Cossa Polimeri ESTASTIR HI 0412 Polystyrene
Polystyrene for injection molding or extrusionHigh impact resistance, good thermal resistanceInformation provided by Cossa Polimeri S.r.l.
Izod Impact, Notched 1.20 - 1.50 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
2.25 - 2.81 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256, ISO 180/4a
EPICHEM Epilac T ABS Acrylonitrile Butadiene Styrene
Izod Impact, Notched 1.20 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
2.25 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256, ISO 180/4a
EPICHEM Epilon G2-PC 10% GF Polycarbonate, 10% Glass Fiber
Characteristics: 10% glass fibre filled, good mechanical properties
Izod Impact, Notched 1.20 J/cm

@Temperature 23.0 °C
2.25 ft-lb/in

@Temperature 73.4 °F
ASTM D256A
Braskem RP 347 Injection Molding Polypropylene
Description: RP 347 is a medium melt flow rate random copolymer designed for injection moulding. This product offers excellent transparency and gloss, very good stiffness/impact strength balance, ex..
Izod Impact, Notched 1.20 J/cm

@Temperature 23.0 °C
2.25 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Carmel Olefins CAPILENE® SL 50 Polypropylene Impact Copolymer
Description: CAPILENE® SL 50 is a medium melt flow rate impact copolymer for injection molding applications. This grade combines good stiffness and impact properties.Applications: CAPILENE® SL ..
Izod Impact, Notched 1.20 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
2.25 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
Asahi Kasei Xyron® X5402 PPE/PA
Oil ResistantInformation provided by Asahi Kasei
Izod Impact, Notched 1.20 J/cm

@Thickness 3.18 mm,
Temperature -18.0 °C
2.25 ft-lb/in

@Thickness 0.125 in,
Temperature -0.400 °F
Compression Molded, all complete breaks; ASTM D256A
PolyOne Geon™ Vinyl Rigid Extrusion L6256 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Copyright © lookpolymers.com All Rights Reserved