Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Notched = 2.22 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 2.22 J/cm

@Thickness 6.35 mm
4.16 ft-lb/in

@Thickness 0.250 in
ASTM D256
Chi Mei Polylac® PA-716 ABS - High Flow
High flow, medium impact
Izod Impact, Notched 2.22 J/cm

@Thickness 3.17 mm
4.16 ft-lb/in

@Thickness 0.125 in
ASTM D256
Chi Mei Polylac® PA-765 ABS - Flame Retardant
F.R. High Flow
Izod Impact, Notched 2.22 J/cm

@Thickness 6.35 mm
4.16 ft-lb/in

@Thickness 0.250 in
ASTM D256
Chi Mei Polylac® PA-765B ABS - Flame Retardant
F.R. Medium Impact
Izod Impact, Notched 2.22 J/cm

@Temperature 23.0 °C
4.16 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics LNP Verton RX93407D PA 66
LNP* Verton* RX93407D is a compound based on Nylon 66 resin.This data was supplied by SABIC-IP for the Americas region.
Copyright © lookpolymers.com All Rights Reserved