Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 2.14 J/cm @Temperature 22.8 °C |
4.00 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources ABS-GP1 General Purpose ABS General Purpose Acrylonitrile Butadiene StyreneFeatures: • Medium Impact ResistanceProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pig.. |
|||
Izod Impact, Notched | 2.14 J/cm @Temperature 22.8 °C |
4.00 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources ABS-GP1-[color]-EP General Purpose ABS, Electroplating Grade General Purpose Acrylonitrile Butadiene Styrene, Electroplating GradeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sam.. |
|||
Izod Impact, Notched | 2.14 J/cm @Temperature 22.8 °C |
4.00 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources ABS-GP1-[color]-UV General Purpose ABS, UV-stabilized General Purpose Acrylonitrile Butadiene Styrene, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.In.. |
|||
Izod Impact, Notched | 2.14 J/cm @Temperature 23.0 °C |
4.00 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Noble Polymers Regis™ 125098 Thermoplastic Olefin (TPO) Regis is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. We have created Regis for use in bumpers and bumper fascias, air dams, exterior panels, materi.. |
|||
Izod Impact, Notched | 2.14 J/cm @Temperature 22.8 °C |
4.00 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources PPX-EN-FR3 Modified-PPO, V-1 Flame Retardant, Extrusion Grade Modified-Polyphenylene Oxide, V-1 Flame Retardant, 265F HDT, Extrusion GradeFeatures: • Bromine Free • Chlorine FreeProcess: ExtrusionNotes: All physical, mechanical and thermal testing conducte.. |
|||
Izod Impact, Notched | 2.14 J/cm @Temperature 22.8 °C |
4.00 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources PPX-FR3 Modified-PPO, V-1 Flame Retardant Modified-Polyphenylene Oxide, V-1 Flame Retardant, 265F HDTFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-.. |
|||
Izod Impact, Notched | 2.14 J/cm @Temperature 22.8 °C |
4.00 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources PPX-GP1 Modified-PPO, General Purpose Modified-Polyphenylene Oxide, General Purpose, 265F HDTFeatures: • Hydrolytically Stable • Low to No Water AbsorptionProcess: Injection MoldingNotes: All physical, mechanical and thermal testing.. |
|||
Izod Impact, Notched | 2.14 J/cm @Temperature 22.8 °C |
4.00 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources PPX-GP1-[color]-EN Modified-PPO, Extrusion Grade Modified-Polyphenylene Oxide, Extrusion Grade, 265F HDTFeatures: • Hydrolytically Stable • Low to No Water AbsorptionProcess: Extrusion Notes: All physical, mechanical and thermal testing conduc.. |
|||
Izod Impact, Notched | 2.14 J/cm @Temperature 22.8 °C |
4.00 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources PPX-GP2 Modified-PPO, General Purpose Modified-Polyphenylene Oxide, General Purpose, 250F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati.. |
|||
Izod Impact, Notched | 2.14 J/cm @Temperature 22.8 °C |
4.00 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources PPX-GP3 Modified-PPO, General Purpose Modified-Polyphenylene Oxide, General Purpose, 235F HDTFeatures: • Hydrolytically Stable • Low to No Water AbsorptionProcess: Injection MoldingNotes: All physical, mechanical and thermal testing.. |
|||
Izod Impact, Notched | 2.14 J/cm @Temperature 22.8 °C |
4.00 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources PPX-GP3-[color]-EN Modified-PPO, Extrusion Grade Modified-Polyphenylene Oxide, Extrusion Grade, 235F HDTFeatures: • Hydrolytically Stable • Low to No Water AbsorptionProcess: ExtrusionNotes: All physical, mechanical and thermal testing conduct.. |
|||
Izod Impact, Notched | 2.14 J/cm @Temperature 22.8 °C |
4.00 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources PPX-GP5 Modified-PPO, General Purpose Modified-Polyphenylene Oxide, General Purpose, 270F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati.. |
|||
Izod Impact, Notched | 2.14 J/cm @Temperature 22.8 °C |
4.00 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources PPX-GP7 Modified-PPO, General Purpose Modified-Polyphenylene Oxide, General Purpose, 300F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati.. |
|||
Izod Impact, Notched | 2.14 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
4.00 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D256 |
Ravago Manufacturing Americas Hybrid B2035I Polycarbonate + PBT Alloy Available in North America High Impact Resistance Form: PelletsInformation provided by Ravago |
|||
Izod Impact, Notched | 2.14 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
4.01 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
notch |
Kraton® G1651 + PC blend (5/95) Blending KRATON D and G polymers with PC significantly improves the toughness at both room and low temperatures. KRATON polymers are block segments of styrene and rubber monomers (A-B, A-B-A, or [A.. |
|||
Izod Impact, Notched | 2.14 J/cm @Temperature -29.0 °C |
4.01 ft-lb/in @Temperature -20.2 °F |
3.2 mm (0.125 in) notch |
Kraton® G1657 + PA-6,6 blend (16/4/80) Blending KRATON D and G polymers with PA significantly improves the toughness at both room and low temperatures. KRATON polymers are block segments of styrene and rubber monomers (A-B, A-B-A, or [A.. |
|||
Izod Impact, Notched | 2.14 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
4.00 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D256 |
Techmer ES Elastoblend® PC IM X Availability: North AmericaForms: PelletsAdditive: Impact Modifier and Mold ReleaseFeatures: Impact Modified and Good Mold ReleaseProcessing Method: Injection MoldingInformation provided by TP Compo.. |
|||
Izod Impact, Notched | 2.14 J/cm @Thickness 6.35 mm, Temperature 22.8 °C |
4.00 ft-lb/in @Thickness 0.250 in, Temperature 73.0 °F |
ASTM D256 |
Techmer ES Elastoblend® PC IM X Availability: North AmericaForms: PelletsAdditive: Impact Modifier and Mold ReleaseFeatures: Impact Modified and Good Mold ReleaseProcessing Method: Injection MoldingInformation provided by TP Compo.. |
|||
Izod Impact, Notched | 2.14 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
4.00 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D256 |
Techmer ES Elastoblend® PC IM Availability: North AmericaForms: PelletsAdditive: Impact Modifier Features: Impact Modified Processing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 2.14 J/cm @Thickness 6.35 mm, Temperature 22.8 °C |
4.00 ft-lb/in @Thickness 0.250 in, Temperature 73.0 °F |
ASTM D256 |
Techmer ES Elastoblend® PC IM Availability: North AmericaForms: PelletsAdditive: Impact Modifier Features: Impact Modified Processing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 2.14 J/cm @Thickness 3.17 mm, Temperature 72.8 °C |
4.00 ft-lb/in @Thickness 0.125 in, Temperature 163 °F |
ASTM D256 |
Techmer ES HiFill FR® PA6/6 GF25 FR-N IM BK 25% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 25% Filler by WeightAdditive: Impact ModifierFeatures: Flame Retardant and Impact ModifiedUL File Number: E157318Appearanc.. |
|||
Izod Impact, Notched | 2.14 J/cm @Temperature 23.0 °C |
4.01 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Eastman Tenite 360E3V45508 Propionate Water Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi.. |
|||
Izod Impact, Notched | 2.14 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
4.01 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Diamond Polymers NPP25-0604 Impact Copolymer Polypropylene Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Izod Impact, Notched | 2.14 J/cm @Temperature 23.0 °C |
4.00 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Dow AFFINITY™ SM 1300G Polyolefin Plastomer (POP) AFFINITY™ SM 1300G is an ethylene alpha-olefin resin for Injection Molding is produced via INSITE™ Technology from Dow Plastics. The resin offers excellent performance in durable injection molded.. |
|||
Izod Impact, Notched | 2.14 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
4.00 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D-256 |
Axiall HH-2000 Rigid PVC, Molding Georgia Gulf HH-2000 is a high heat/high flow injection molding grade PVC alloy with a price/performance niche between high flow vinyl and utility engineering thermoplastics. It combines excellent .. |
|||
Izod Impact, Notched | 2.14 J/cm @Thickness 3.17 mm |
4.00 ft-lb/in @Thickness 0.125 in |
ASTM D-256 |
Axiall 7751 Rigid PVC, Extrusion Georgia Gulf 7751 is a vertical blind profile exterior compound requiring the following properties: Impact Strength & ToughnessColorabilityDimensional StabilityUV Color StabilityEasy Processing in .. |
|||
Izod Impact, Notched | 2.14 J/cm @Thickness 6.35 mm, Temperature -28.9 °C |
4.00 ft-lb/in @Thickness 0.250 in, Temperature -20.0 °F |
ASTM D-256 |
Axiall 7801 Rigid PVC, Extrusion, White, High Impact Profile Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Izod Impact, Notched | 2.14 J/cm @Thickness 6.35 mm, Temperature -28.9 °C |
4.00 ft-lb/in @Thickness 0.250 in, Temperature -20.0 °F |
ASTM D-256 |
Axiall 7803 Rigid PVC, Extrusion High Impact Profile Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Izod Impact, Notched | >= 2.14 J/cm @Temperature 23.0 °C |
>= 4.00 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Buckeye Polymers BP FLEX D5518 R 848 Thermoplastic Polyolefin Product Information: TPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment.Product Features:High tear resist.. |
|||
Izod Impact, Notched | 2.14 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
4.00 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D256 |
Techmer ES Luriblend® ABS TL10 Availability: North AmericaForms: PelletsAdditive: PTFE LubricantFeatures: LubricatedInformation provided by TP Composites, Inc. |