Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 2.00 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
3.75 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Compression Molded, Across Flow; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Extrusion 85857 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Izod Impact, Notched | 2.00 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
3.75 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Compression Molded, Flow; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Extrusion 87180 Polyvinyl Chloride, Rigid (PVC, Rigid) Note: NSF listings are obtained on specific colors. Contact PolyOne for the latest listing of approved colors for this product. Note: The Cell Classification was determined using the notched Izod te.. |
|||
Izod Impact, Notched | 2.00 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
3.75 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Compression Molded, Across Flow; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Extrusion 87759 Polyvinyl Chloride, Rigid (PVC, Rigid) Note: Finished part testing is required for ASTM E-84 certification. Note: The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by Po.. |
|||
Izod Impact, Notched | 2.00 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
3.75 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Compression Molded, Across Flow; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Extrusion L4857 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Izod Impact, Notched | 2.00 J/cm @Thickness 3.18 mm, Temperature 0.000 °C |
3.75 ft-lb/in @Thickness 0.125 in, Temperature 32.0 °F |
Compression Molded; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Extrusion L7801 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Izod Impact, Notched | 2.00 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
3.75 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ISO 180/4A |
Polimeri Europa Sinkral® C 442 ABS Resin Sinkral C 442 is a heat resistant injection molding grade offering good flow and impact resistance together with excellent thermal stability during processing. Designation: Thermoplastic ISO 2580-AB.. |
|||
Izod Impact, Notched | 2.00 J/cm @Temperature -30.0 °C |
3.75 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® FXD9810U PC Copolymer (Asia Pacific) Polycarbonate with high flow, excellent processability, good impact and thermal properties, UV stabilized, non-Chlorine and non-Bromine flame retardant, UL rated V-0 and V-1. Available in limited di.. |
|||
Izod Impact, Notched | 2.00 J/cm @Temperature 23.0 °C |
3.75 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Noryl V0150BT PPE+HIPS Noryl* V0150BT is an unfilled, injection moldable modified polyphenylene ether resin.. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 1.5 mm .. |
|||
Izod Impact, Notched | 2.00 J/cm @Temperature 23.0 °C |
3.75 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Noryl V0150BT PPE+HIPS (Asia Pacific) Noryl* V0150BT is an unfilled, injection moldable modified polyphenylene ether resin.. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 1.5 mm .. |
|||
Izod Impact, Notched | 2.00 J/cm @Temperature 23.0 °C |
3.75 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Noryl V0150BT PPE+HIPS (Europe-Africa-Middle East) Noryl* V0150BT is an unfilled, injection moldable modified polyphenylene ether resin.. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 1.5 mm .. |
|||
Izod Impact, Notched | 2.00 J/cm @Thickness 3.20 mm, Temperature -18.0 °C |
3.75 ft-lb/in @Thickness 0.126 in, Temperature -0.400 °F |
Injection Molded; ASTM D256 |
Styron EMERGEâ„¢ 7700 Polycarbonate (PC) / Acrylonitrile Butadiene Styrene (ABS) Overview: EMERGEâ„¢ PC/ABS 7700 Advanced Resin is an ignition-resistant PC/ABS blend that contains no chlorine for bromine additives. It has superior processability for injection molding applicat.. |
|||
Izod Impact, Notched | 2.00 J/cm @Temperature 23.0 °C |
3.75 ft-lb/in @Temperature 73.4 °F |
Practical Use (Water Absorption 2.5%); ASTM-D256 |
Toyobo GLAMIDE® T-402 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Izod Impact, Notched | 2.00 J/cm @Temperature 23.0 °C |
3.75 ft-lb/in @Temperature 73.4 °F |
Practical Use (Water Absorption 1.7%); ASTM-D256 |
Toyobo GLAMIDE® NB-5550 Nylon/Olefin GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Izod Impact, Notched | 2.00 J/cm @Temperature 23.0 °C |
3.75 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
Cossa Polimeri ESTADIENE 0420 HHT Acrylonitrile Butadiene Styrene ABS for injection molding or extrusionVery high thermal resistance, good impact resistanceInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 2.00 J/cm @Temperature 23.0 °C |
3.75 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
Cossa Polimeri ESTADIENE 0820 HT Acrylonitrile Butadiene Styrene ABS with high thermal resistanceGood impact resistance, stiffness, high gloss, with antistatic, excellent processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 2.00 J/cm @Temperature 23.0 °C |
3.75 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
Cossa Polimeri ESTADIENE 1020 HHT Acrylonitrile Butadiene Styrene ABS with very high heat resistanceGood melt flow rate, good impact resistance, stiff, excellent surface appearance, good processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 2.00 J/cm @Temperature 23.0 °C |
3.75 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
Cossa Polimeri ESTADIENE 2020 MT Acrylonitrile Butadiene Styrene ABSMedium heat resistance, good impact resistance, good melt flow rate, high gloss, with antistatic, excellent processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 2.00 J/cm @Temperature 0.000 °C |
3.75 ft-lb/in @Temperature 32.0 °F |
ASTM D 638 |
Cossa Polimeri ESTADIENE 2525 AS Acrylonitrile Butadiene Styrene ABS with high impact resistanceGood melt flow rate, with antistatic, excellent processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 2.00 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
3.75 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256, ISO 180/4a |
EPICHEM Epiryl PPO V0 Polyphenylene oxide Characteristics: self-extinguishing V0 at 1,6 mm |
|||
Izod Impact, Notched | 2.00 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
3.75 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Compression Molded, Flow; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Extrusion L6181 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |