Polymer Property : Izod Impact, Notched = 15.6 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 8.34 J/cm

@Thickness 3.17 mm
15.6 ft-lb/in

@Thickness 0.125 in
ASTM D256
Samsung Cheil Industries Infino® EF-1032 PC/ABS, Unreinforced FR
Extrusion resin, non-halogen flame-retardantInformation provided by Samsung Cheil Industries.
Izod Impact, Notched 8.34 J/cm

@Thickness 3.17 mm
15.6 ft-lb/in

@Thickness 0.125 in
ASTM D256
Samsung Cheil Industries Infino® EF-1032 PC/ABS, Unreinforced FR
Extrusion resin, non-halogen flame-retardantInformation provided by Samsung Cheil Industries.