Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 6.35 J/cm @Temperature 0.000 °C |
11.9 ft-lb/in @Temperature 32.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Geloy XTPM309 ASA+PC (Europe-Africa-Middle East) XTPM309 is a modified HRA170 with improved processing stability.Typical properties measured on natural material.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Notched | 6.35 J/cm @Temperature 23.0 °C |
11.9 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOY HR-5006A Heat Resistant PC/ABS Alloy, Unreinforced, Weather Resistant Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive.. |
|||
Izod Impact, Notched | >= 6.37 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
>= 11.9 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOY HR5007A PC/ABS, Heat Resistance, High Impact Description: Injection Molding, PC/ABS, Heat Resistance, High Flow, High Impact.Application: Automotive (Interior), E&E (housing)CAS: 103598-77-2 and 9003-56-9Information provided by LG Chemical |
|||
Izod Impact, Notched | 6.35 J/cm @Temperature 23.0 °C |
11.9 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOY HR-5007AX Heat Resistant PC/ABS Alloy, Unreinforced Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive.. |
|||
Izod Impact, Notched | >= 6.37 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
>= 11.9 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOY SC1004L PC, High Impact Description: Injection Molding, PC, General Purpose, High Flow, High Impact, Chemical ResistanceApplication: Mobile Phone HousingInformation provided by LG Chemical |
|||
Izod Impact, Notched | 6.35 J/cm @Temperature 23.0 °C |
11.9 ft-lb/in @Temperature 73.4 °F |
3.2 mm (0.125 in) notch |
Kraton® G1651 + PPE blend (20/80) Blending KRATON D and G polymers with PPE significantly improves the toughness at both room and low temperatures. KRATON polymers are block segments of styrene and rubber monomers (A-B, A-B-A, or [.. |
|||
Izod Impact, Notched | 6.37 J/cm @Thickness 3.17 mm |
11.9 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® TP-1002 PC, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 6.37 J/cm @Thickness 3.17 mm |
11.9 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® TP-1020 PC, Unreinforced Transparent Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 6.37 J/cm @Thickness 3.17 mm |
11.9 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® TP-1002 PC, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 6.37 J/cm @Thickness 6.35 mm |
11.9 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Infino® HN-1064IA PC, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 6.37 J/cm @Thickness 3.17 mm |
11.9 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® TP-1020 PC, Unreinforced Transparent Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 6.37 J/cm @Thickness 3.20 mm |
11.9 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Bhansali Engineering Abstron IMC-45V ABS-PC Alloy ABS-polycarbonate alloys for High service temperature applications.Information provided by Bhansali |
|||
Izod Impact, Notched | 6.37 J/cm @Thickness 3.20 mm |
11.9 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Bhansali Engineering Abstron IMC-45V ABS-PC Alloy ABS-polycarbonate alloys for High service temperature applications.Information provided by Bhansali |
|||
Izod Impact, Notched | 6.37 J/cm @Thickness 6.35 mm |
11.9 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Infino® HN-1064IA PC, Unreinforced FR Information provided by Samsung Cheil Industries. |