Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 5.90 J/cm @Thickness 3.18 mm, Temperature 0.000 °C |
11.1 ft-lb/in @Thickness 0.125 in, Temperature 32.0 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Molding M3890 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Izod Impact, Notched | 5.90 J/cm @Thickness 3.18 mm, Temperature 0.000 °C |
11.1 ft-lb/in @Thickness 0.125 in, Temperature 32.0 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Molding M3900 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Izod Impact, Notched | 5.90 J/cm @Thickness 3.18 mm, Temperature 0.000 °C |
11.1 ft-lb/in @Thickness 0.125 in, Temperature 32.0 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Molding M4885 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Izod Impact, Notched | 5.90 J/cm @Temperature 23.0 °C |
11.1 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycoloy® CU1650 PC+ABS (Europe-Africa-Middle East) UV stabilized, non-FR PC/ABS of excellent flow and impact performanceThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Notched | 5.90 J/cm @Temperature 23.0 °C |
11.1 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycoloy® CY9650 PC+ABS PC+ABS, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat AgingThis data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 5.90 J/cm @Temperature 23.0 °C |
11.1 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycoloy® CY9650 PC+ABS (Asia Pacific) PC+ABS, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat AgingThis data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 5.90 J/cm @Temperature 23.0 °C |
11.1 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycoloy® CY9650 PC+ABS (Europe-Africa-Middle East) PC+ABS, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat AgingThis data was supplied by SABIC-IP for the Europe-Africa-Middle East re.. |
|||
Izod Impact, Notched | 5.90 J/cm @Temperature 23.0 °C |
11.1 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycoloy® XCY630 PC+ABS (Europe-Africa-Middle East) PC+ ABS Automotive applications, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat AgingThis data was supplied by SABIC-IP for the Eur.. |
|||
Izod Impact, Notched | 5.90 J/cm @Thickness 3.18 mm, Temperature 0.000 °C |
11.1 ft-lb/in @Thickness 0.125 in, Temperature 32.0 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ HTX M6307 Polyvinyl Chloride Alloy (PVC Alloy) Information provided by PolyOne |
|||
Izod Impact, Notched | 5.95 J/cm @Temperature 0.000 °C |
11.1 ft-lb/in @Temperature 32.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Geloy XTPM307 ASA+PC (Europe-Africa-Middle East) XTPM307 is a high heat resistant PC/ASA with improved processing stability over HRA150. Typical values measured on natural material.This data was supplied by SABIC-IP for the Europe-Africa-Middle Ea.. |
|||
Izod Impact, Notched | 5.90 J/cm @Temperature 23.0 °C |
11.1 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOY HF-5000 High Flow PC/ABS Alloy, Unreinforced Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive.. |
|||
Izod Impact, Notched | 5.90 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
11.1 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
Injection Molded; ASTM D256 |
Styron EMERGEâ„¢ 7700 Polycarbonate (PC) / Acrylonitrile Butadiene Styrene (ABS) Overview: EMERGEâ„¢ PC/ABS 7700 Advanced Resin is an ignition-resistant PC/ABS blend that contains no chlorine for bromine additives. It has superior processability for injection molding applicat.. |