Polymer Property : Izod Impact, Notched = 11.0 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 11.0 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
20.6 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Compression Molded, Across Flow; ASTM D256A
PolyOne Geon™ Vinyl Rigid Extrusion 85880 Polyvinyl Chloride, Rigid (PVC, Rigid)
The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne
Izod Impact, Notched 11.0 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
20.6 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
PolyOne Geon™ Vinyl Rigid Extrusion 8700X Polyvinyl Chloride, Rigid (PVC, Rigid)
Note: Automotive OEM approval(s). Note: NSF listings are obtained on specific colors. Contact PolyOne for the latest listing of approved colors for this product. Note: The Cell Classification was de..
Izod Impact, Notched 11.0 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
20.6 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Compression Molded, Across Flow; ASTM D256A
PolyOne Geon™ Vinyl Rigid Extrusion 8700X Polyvinyl Chloride, Rigid (PVC, Rigid)
Note: Automotive OEM approval(s). Note: NSF listings are obtained on specific colors. Contact PolyOne for the latest listing of approved colors for this product. Note: The Cell Classification was de..
Izod Impact, Notched 11.0 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
20.6 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
PolyOne Geon™ Vinyl Rigid Extrusion 87150 Polyvinyl Chloride, Rigid (PVC, Rigid)
Note: NSF listings are obtained on specific colors. Contact PolyOne for the latest listing of approved colors for this product. Note: The Cell Classification was determined using the notched Izod te..
Izod Impact, Notched 11.0 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
20.6 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Compression Molded, Across Flow; ASTM D256A
PolyOne Geon™ Vinyl Rigid Extrusion 87262 Polyvinyl Chloride, Rigid (PVC, Rigid)
The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne
Izod Impact, Notched 11.0 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
20.6 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
PolyOne Geon™ Vinyl Rigid Extrusion 87547 Polyvinyl Chloride, Rigid (PVC, Rigid)
The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne
Izod Impact, Notched 11.0 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
20.6 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
PolyOne Geon™ Vinyl Rigid Extrusion 87548 AS Polyvinyl Chloride, Rigid (PVC, Rigid)
A transparent PVC profile compound, with reduced surface resistivity, resulting in unlikely attraction and adhesion of dust. Actual results on surface resistivity = 1.3x10^15.Information provided by..
Izod Impact, Notched 11.0 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
20.6 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
PolyOne Geon™ Vinyl Rigid Extrusion 87548 Polyvinyl Chloride, Rigid (PVC, Rigid)
A transparent PVC profile compound, with inherent water clear optical characteristics.Information provided by PolyOne
Izod Impact, Notched 11.0 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
20.6 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
PolyOne Geon™ Vinyl Rigid Extrusion 87549 Polyvinyl Chloride, Rigid (PVC, Rigid)
The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne
Izod Impact, Notched 11.0 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
20.6 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
PolyOne Geon™ Vinyl Rigid Extrusion 87554 Polyvinyl Chloride, Rigid (PVC, Rigid)
The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne
Izod Impact, Notched 11.0 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
20.6 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
PolyOne Geon™ Vinyl Rigid Extrusion 87555 Polyvinyl Chloride, Rigid (PVC, Rigid)
The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne
Izod Impact, Notched 11.0 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
20.6 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
PolyOne Geon™ Vinyl Rigid Extrusion 87556 Polyvinyl Chloride, Rigid (PVC, Rigid)
The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne
Izod Impact, Notched 11.0 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
20.6 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Compression Molded, Flow; ASTM D256A
PolyOne Geon™ Vinyl Rigid Extrusion L0248 Opaque Polyvinyl Chloride, Rigid (PVC, Rigid)
The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne
Izod Impact, Notched 11.0 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
20.6 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Compression Molded, Across Flow; ASTM D256A
PolyOne Geon™ Vinyl Rigid Extrusion L0248 Polyvinyl Chloride, Rigid (PVC, Rigid)
The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne
Izod Impact, Notched 11.0 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
20.6 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
PolyOne Geon™ Vinyl Rigid Extrusion L0659 Polyvinyl Chloride, Rigid (PVC, Rigid)
The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne
Izod Impact, Notched 11.0 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
20.6 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Compression Molded, Flow; ASTM D256A
PolyOne Geon™ Vinyl Rigid Extrusion L0676 Polyvinyl Chloride, Rigid (PVC, Rigid)
Note: NSF listings are obtained on specific colors. Contact PolyOne for the latest listing of approved colors for this product. Note: The Cell Classification was determined using the notched Izod te..
Izod Impact, Notched 11.0 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
20.6 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
PolyOne Geon™ Vinyl Rigid Extrusion L0678 Natural Polyvinyl Chloride, Rigid (PVC, Rigid)
The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne
Izod Impact, Notched 11.0 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
20.6 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Compression Molded; ASTM D256A
PolyOne Geon™ Vinyl Rigid Extrusion L7801 Polyvinyl Chloride, Rigid (PVC, Rigid)
The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne
Izod Impact, Notched 11.0 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
20.6 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
PolyOne Geon™ Vinyl Rigid Molding 6957 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Izod Impact, Notched 11.0 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
20.6 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
PolyOne Geon™ Vinyl Rigid Molding M5200 Natural Polyvinyl Chloride, Rigid (PVC, Rigid)
NOTE: Geon weatherable compounds contain pigments and ingredients that, along with processing conditions, contribute to the weathering performance of the PVC compounds. The weathering performance of..
Izod Impact, Notched 11.0 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
20.6 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
PolyOne Geon™ Vinyl Fittings 87322 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Izod Impact, Notched 11.0 J/cm

@Temperature 23.0 °C
20.6 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Solvay Specialty Polymers Amodel® AT-1001L Polyphthalamide (PPA)
Amodel® AT-1001L is an unreinforced, impact modified polyphthalamide (PPA) resin that exhibits exceptional impact strength at temperatures ranging from room temperature to as low as -40°F (-40..
Izod Impact, Notched 11.0 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
20.6 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Compression Molded, Across Flow; ASTM D256A
PolyOne Geon™ Vinyl Rigid Extrusion L5880 Polyvinyl Chloride, Rigid (PVC, Rigid)
The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne
Izod Impact, Notched 11.0 J/cm

@Temperature 23.0 °C
20.6 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Solvay Specialty Polymers Amodel® AT-1001L Polyphthalamide (PPA)  (Unverified Data**)
Amodel AT-1001L is an unreinforced, impact modified polyphthalamide (PPA) resin that exhibits exceptional impact strength at temperatures ranging from room temperature to as low as -40°F (-40°C), ..
Izod Impact, Notched 11.0 J/cm

@Temperature 23.0 °C
20.6 ft-lb/in

@Temperature 73.4 °F
Conditioned; ASTM D256
Solvay Specialty Polymers Amodel® ET-1000 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel ET-1000 HS is an impact modified, heat stabilized polyphthalamide (PPA) that exhibits exceptional impact strength and toughness. Like all Amodel PPA resins, ET-1000 HS offers high fatigue str..