Polymer Property : Izod Impact, Notched = 10.6 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 5.66 J/cm

@Temperature 23.0 °C
10.6 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics Lexan® ML6018R PC (Asia Pacific)
ML6018R is a low viscosity grade exhibiting a high impact performance over standard PC. It contains an enhanced release-agent. Opaque colours only.This data was supplied by SABIC-IP for the Asia Pac..