Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.940 J/cm @Thickness 4.00 mm, Temperature 23.0 °C |
1.76 ft-lb/in @Thickness 0.157 in, Temperature 73.4 °F |
ISO 180 |
Premix Thermoplastics PRE-ELEC® PP 1375 PRE-ELEC PP 1375 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELE.. |
|||
Izod Impact, Notched | 0.940 J/cm @Temperature 23.0 °C |
1.76 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Eastman Provista MP001 Copolymer Provista Copolymer MP001 is a resin specifically developed for extrusion into profiles where aesthetics such as high clarity and gloss, coupled with design flexibility, drive demand. Compared to com.. |
|||
Izod Impact, Notched | 0.940 J/cm @Temperature 23.0 °C |
1.76 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Eastman Provista UVI Copolymer Provista UVI is a Provista copolymer with an indoor/outdoor UV package added to prevent yellowing caused by light. Provista copolymer is a resin specifically developed for extrusion into profiles wh.. |
|||
Izod Impact, Notched | 0.940 J/cm @Temperature 23.0 °C |
1.76 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Eastman Provista UVO Copolymer Provista UVO is a Provista copolymer with an indoor/outdoor UV package added to prevent yellowing caused by light. Provista copolymer is a resin specifically developed for extrusion into profiles wh.. |
|||
Izod Impact, Notched | 0.940 J/cm @Temperature 23.0 °C |
1.76 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Eastman Eastar GN046 Copolyester, Natural Eastar Copolyester GN046 is a very high melt strength copolyester targeted for extrusion blow molding applications. Blow molding of large parts (up to several pounds) are possible with this material.. |