Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.883 J/cm @Temperature 23.0 °C |
1.65 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
PolyMirae Moplen EP640R Injection Molding Grade Polypropylene Moplen EP640R is the polypropylene block copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen EP640R is a block copolymer particularly suitable for injection.. |
|||
Izod Impact, Notched | 0.883 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
1.65 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical HIPS 403AF PS, Flame Retardant Description: Injection Molding, PS, Flame RetardantApplication: Electric Parts Requiring Flame RetardancyCAS: 9003-55-8, 21850-44-2 and 1309-64-4Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.883 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
1.65 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical HIPS 410AF PS, Flame Retardant Description: Injection Molding, PS, Flame RetardantApplication: Office Appliances (Parts of Printer or Copier)CAS: 9003-55-8, 25713-60-4 and 1309-64-4Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.883 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
1.65 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical HIPS 460AF PS, Flame Retardant Description: Injection Molding, PS, Flame RetardantApplication: Electric Parts Requiring Flame RetardancyCAS: 9003-55-8, 25713-60-4, 84852-53-9 and 1309-64-4Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.883 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
1.65 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical HIPS 60HRI PS, Impact Modified Description: Injection Molding, PS, General Purpose, Impact ModifiedApplication: TV Sets, Tape Recorders, Vacuum Cleaner, Washing Machine, Air ConditionerCAS: 9003-55-8Information provided by LG Che.. |
|||
Izod Impact, Notched | 0.883 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
1.65 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical HIPS 65IHE PS, Impact Modified Description: Injection Molding, PS, General Purpose, Impact ModifiedApplication: Refrigerator Tray, Food Tray, Refrigerator Door LinerCAS: 9003-55-8Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.883 J/cm @Thickness 6.50 mm, Temperature 23.0 °C |
1.65 ft-lb/in @Thickness 0.256 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LI942 Heat Resistant ASA Description: High Heat ASAApplication: Automotive Part (Roof Rack Cover)CAS: 26299-47-8Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.883 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
1.65 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LI942 Heat Resistant ASA Description: High Heat ASAApplication: Automotive Part (Roof Rack Cover)CAS: 26299-47-8Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.880 J/cm @Thickness 3.17 mm |
1.65 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
LG Chemical 401 AF Flame Retardant HIPS NON-DECA, Flame retardant, Safety standards: listed with UL CSA, and classified according to IEC 707, Meet requirements for flammability, mechanical and electrical properties, uses non-bromide as fl.. |
|||
Izod Impact, Notched | 0.883 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
1.65 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical AF305HT ABS, Flame Retardant, Heat Resistance Feature: Injection Molding, Flame Retardant, Heat ResistanceApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 9001-96-2, 68928-70-1, and 1309-64-4Inf.. |
|||
Izod Impact, Notched | 0.883 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
1.65 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical XG568 MABS, Anti-Scratch, High Gloss Feature: Injection Molding, Anti-Scratch, High GlossApplication: LCD TV Front Cabinet, Bezel, Audio/Video HousingCSA No. 9011-14-7 and 9003-56-9Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.883 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
1.65 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical XG568 MABS, Anti-Scratch, High Gloss Feature: Injection Molding, Anti-Scratch, High GlossApplication: LCD TV Front Cabinet, Bezel, Audio/Video HousingCSA No. 9011-14-7 and 9003-56-9Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.883 J/cm @Thickness 6.35 mm |
1.65 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Infino® AR-6508 PBT/PET, Glass Filled Good WeatherabilityInformation provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.883 J/cm @Thickness 6.35 mm |
1.65 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Starex® BF-0677HF MABS, Unreinforced Scratch Resistant Scratch resistant material that is used in TV housing and the exterior material for cleaner and air purifierInformation provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.883 J/cm @Thickness 3.17 mm |
1.65 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® GR-4010 ABS, 10% Glass Filled Material with 10% GF reinforcement with high stiffness that can be used in refrigerator vegetable boxesInformation provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.883 J/cm @Thickness 3.17 mm, Temperature -30.0 °C |
1.65 ft-lb/in @Thickness 0.125 in, Temperature -22.0 °F |
ASTM D256 |
Samsung Cheil Industries Starex® MP-0670 ABS, Metal Plating Grade Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.883 J/cm @Thickness 6.35 mm |
1.65 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Starex® BF-0677HF MABS, Unreinforced Scratch Resistant Scratch resistant material that is used in TV housing and the exterior material for cleaner and air purifierInformation provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.883 J/cm @Thickness 3.17 mm |
1.65 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® GR-4010 ABS, 10% Glass Filled Material with 10% GF reinforcement with high stiffness that can be used in refrigerator vegetable boxesInformation provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.883 J/cm @Thickness 3.17 mm, Temperature -30.0 °C |
1.65 ft-lb/in @Thickness 0.125 in, Temperature -22.0 °F |
ASTM D256 |
Samsung Cheil Industries Starex® MP-0670 ABS, Metal Plating Grade Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.880 J/cm @Temperature 23.0 °C |
1.65 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Xylex FXY391DF PC+POLYESTER (Asia Pacific) PC+Polyester alloy in Diffusion Visual fx. This grade is compliant with US FDA/European food contact regulations. Color package may influence performance.This data was supplied by SABIC-IP for the A.. |
|||
Izod Impact, Notched | 0.883 J/cm @Thickness 6.35 mm |
1.65 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Infino® AR-6508 PBT/PET, Glass Filled Good WeatherabilityInformation provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.880 J/cm @Temperature 23.0 °C |
1.65 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Eastman Spectar® 14471 Copolyester Spectar copolyester extrudes into plastic sheet that is sparkling clear, tough, chemically resistant, odor-free, versatile, easy to work with and affordable. Its toughness allows fabricators to use .. |
|||
Izod Impact, Notched | 0.880 J/cm @Temperature 23.0 °C |
1.65 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Xylex FXY391DF PC+POLYESTER (Europe-Africa-Middle East) PC+Polyester alloy in Diffusion Visual fx. This grade is compliant with US FDA/European food contact regulations. Color package may influence performance.This data was supplied by SABIC-IP for the E.. |
|||
Izod Impact, Notched | 0.883 - 1.08 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
1.65 - 2.02 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D256 |
Samyang Triel® 5650 Thermoplastics Polyetherester Elastomer, General Extrusion Excellent mechanical characteristics, elasticity, thermal resistance and chemical resistance.5650 is an extrusion grade.Information provided by Samyang. |