Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.677 J/cm @Thickness 6.35 mm |
1.27 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Starex® GR-4020L ABS, Glass Filled ABS/GF material that is used in printer LBP fuserInformation provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.677 J/cm @Thickness 6.35 mm |
1.27 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Starex® GR-4020L ABS, Glass Filled ABS/GF material that is used in printer LBP fuserInformation provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.680 J/cm @Temperature -40.0 °C |
1.27 ft-lb/in @Temperature -40.0 °F |
Practical Use (Water Absorption 2.7%); ASTM-D256 |
Toyobo GLAMIDE® TY-145TZ Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |