Mechanical Properties Metric English Comments
Izod Impact, Notched 1.25 J/cm

@Thickness 3.20 mm,
Temperature -20.0 °C
2.34 ft-lb/in

@Thickness 0.126 in,
Temperature -4.00 °F
ISO 180/4A
Polimeri Europa Sinkral® B 432/E ABS Resin
Sinkral B 432/E is a general purpose extrusion grade which exhibits a good balance between rigidity and toughness. Designation: Thermoplastic ISO 2580-ABS 1,EGN,105-04-16-20Applications: Large sheet..
Izod Impact, Notched 1.25 J/cm

@Thickness 3.20 mm,
Temperature -40.0 °C
2.34 ft-lb/in

@Thickness 0.126 in,
Temperature -40.0 °F
ISO 180/4A
Polimeri Europa Sinkral® B 532/E ABS Resin
Sinkral B 532/E is an extrusion grade, which combines high toughness with good rigidity. Its rheological characteristics and good thermal stability are required for the production of large extruded ..
Izod Impact, Notched 1.25 J/cm

@Thickness 3.20 mm,
Temperature -20.0 °C
2.34 ft-lb/in

@Thickness 0.126 in,
Temperature -4.00 °F
ISO 180/4A
Polimeri Europa Sinkral® C 442 ABS Resin
Sinkral C 442 is a heat resistant injection molding grade offering good flow and impact resistance together with excellent thermal stability during processing. Designation: Thermoplastic ISO 2580-AB..
Izod Impact, Notched 1.25 J/cm

@Thickness 3.20 mm,
Temperature 0.000 °C
2.34 ft-lb/in

@Thickness 0.126 in,
Temperature 32.0 °F
ISO 180/4A
Polimeri Europa Sinkral® F 332 ABS Resin
Sinkral F 332 is a general purpose injection molding grade which combines excellent thermal stability during processing with a good balance between flow and impact characteristics. Designation: Ther..
Izod Impact, Notched 1.25 J/cm

@Temperature -30.0 °C
2.34 ft-lb/in

@Temperature -22.0 °F
ASTM D 256
SABIC Innovative Plastics Lexan® 4301 PPC+PC (Asia Pacific)
Lexan 4301 is a high heat resistant poly (ester) carbonate resin for injection moldingThis data was supplied by SABIC-IP for the Asia Pacific region.
Izod Impact, Notched 1.25 J/cm

@Temperature -30.0 °C
2.34 ft-lb/in

@Temperature -22.0 °F
ASTM D 256
SABIC Innovative Plastics Lexan® 4301 PPC+PC (Europe-Africa-Middle East)
Lexan 4301 is a high heat resistant poly (ester) carbonate resin for injection moldingThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Izod Impact, Notched 1.25 J/cm

@Temperature -30.0 °C
2.34 ft-lb/in

@Temperature -22.0 °F
ASTM D 256
SABIC Innovative Plastics Lexan® AD4820 PC
LEXAN AD4820 is a high viscosity grade exhibiting low dust attraction with a UV cut-off up to 400 nm and greater optical purity than standard resin.This data was supplied by SABIC-IP for the America..
Izod Impact, Notched 1.25 J/cm

@Temperature -30.0 °C
2.34 ft-lb/in

@Temperature -22.0 °F
ASTM D 256
SABIC Innovative Plastics Lexan® 4301 PPC+PC
Lexan 4301 is a high heat resistant poly (ester) carbonate resin for injection moldingThis data was supplied by SABIC-IP for the Americas region.
Izod Impact, Notched 1.25 J/cm

@Thickness 6.40 mm,
Temperature 23.0 °C
2.34 ft-lb/in

@Thickness 0.252 in,
Temperature 73.4 °F
ASTM D256
Kingfa NH-627 Flame Retardant ABS
Features:UL 94 V-2 @ 1.6mmHalogen-free flame retardantHigh flowApplications:OA deviceDigital cameraVidiconInformation Provided by Kingfa Sci. & Tech. Co., Ltd.
Izod Impact, Notched 1.25 J/cm

@Temperature 23.0 °C
2.34 ft-lb/in

@Temperature 73.4 °F
Absolute Drying; ASTM-D256
Toyobo GLAMIDE® T-602G30 MXD66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Izod Impact, Notched 1.25 J/cm

@Thickness 3.20 mm,
Temperature -30.0 °C
2.34 ft-lb/in

@Thickness 0.126 in,
Temperature -22.0 °F
ASTM D256, ISO 180/4a
EPICHEM Epiryl B PPO Polyphenylene oxide
Izod Impact, Notched 1.25 J/cm

@Temperature -20.0 °C
2.34 ft-lb/in

@Temperature -4.00 °F
ASTM D256
Carmel Olefins CAPILENE® TG 50 Polypropylene Impact Copolymer
Description: CAPILENE® TG 50 is a heterophasic copolymer designed for injection molding applications requiring optimal impact resistance. This grade combines excellent impact strength, even at lo..