Polymer Property : Izod Impact, Notched = 1.23 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 1.23 J/cm

@Thickness 3.17 mm,
Temperature -40.0 °C
2.30 ft-lb/in

@Thickness 0.125 in,
Temperature -40.0 °F
ASTM D256
Techmer ES Plastiblend® ABS 8003
Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and Impact ModifierFeatures: Heat Stabilized and Impact ModifiedProcessing Method: Injection MoldingInformation provided by TP Comp..
Izod Impact, Notched 1.23 J/cm

@Thickness 3.17 mm,
Temperature -40.0 °C
2.30 ft-lb/in

@Thickness 0.125 in,
Temperature -40.0 °F
ASTM D256
Techmer ES Plastiblend® ABS 8004 FR
Availability: North AmericaForms: PelletsFeatures: Flame RetardantProcessing Method: ExtrusionInformation provided by TP Composites, Inc.
Izod Impact, Notched 1.23 J/cm

@Thickness 3.17 mm,
Temperature -40.0 °C
2.30 ft-lb/in

@Thickness 0.125 in,
Temperature -40.0 °F
ASTM D256
Techmer ES Plastiblend® ABS 8004 UV
Availability: North AmericaForms: PelletsAdditive: UV StabilizerFeatures: Good UV Resistance and High Heat ResistanceInformation provided by TP Composites, Inc.
Izod Impact, Notched 1.23 J/cm

@Thickness 3.17 mm,
Temperature -40.0 °C
2.30 ft-lb/in

@Thickness 0.125 in,
Temperature -40.0 °F
ASTM D256
Techmer ES Plastiblend® ABS 8004 UV MB
Availability: North AmericaForms: PelletsAdditive: UV StabilizerFeatures: Good UV Resistance and High Heat ResistanceTPCI# 6816121Information provided by TP Composites, Inc.
Izod Impact, Notched 1.23 J/cm

@Thickness 3.17 mm,
Temperature -40.0 °C
2.30 ft-lb/in

@Thickness 0.125 in,
Temperature -40.0 °F
ASTM D256
Techmer ES Plastiblend® ABS 8012
Availability: North AmericaForms: PelletsProcessing Method: ExtrusionInformation provided by TP Composites, Inc.
Izod Impact, Notched 1.23 J/cm

@Thickness 3.17 mm,
Temperature -40.0 °C
2.30 ft-lb/in

@Thickness 0.125 in,
Temperature -40.0 °F
ASTM D256
Techmer ES Plastiblend® ABS 8014
Availability: North AmericaForms: PelletsProcessing Method: ExtrusionInformation provided by TP Composites, Inc.
Izod Impact, Notched 1.23 J/cm

@Thickness 3.17 mm,
Temperature -40.0 °C
2.30 ft-lb/in

@Thickness 0.125 in,
Temperature -40.0 °F
ASTM D256
Techmer ES Plastiblend® ABS 8004
Availability: North AmericaForms: PelletsFeatures: General Purpose and High Impact ResistanceInformation provided by TP Composites, Inc.
Izod Impact, Notched 1.23 J/cm

@Thickness 3.17 mm,
Temperature -40.0 °C
2.30 ft-lb/in

@Thickness 0.125 in,
Temperature -40.0 °F
ASTM D256
Techmer ES Plastiblend® ABS FR IM
Availability: North AmericaForms: PelletsFeatures: Flame Retardant and High Impact ResistanceProcessing Method: Injection MoldingInformation provided by TP Composites, Inc.
Izod Impact, Notched 1.23 J/cm

@Thickness 3.17 mm,
Temperature -40.0 °C
2.30 ft-lb/in

@Thickness 0.125 in,
Temperature -40.0 °F
ASTM D256
Techmer ES Plastiblend® ABS IM
Availability: North AmericaForms: PelletsFeatures: High Heat ResistanceInformation provided by TP Composites, Inc.
Izod Impact, Notched 1.23 J/cm

@Temperature -40.0 °C
2.30 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Eastman Tenite 360A4861316 Propionate Clear, Trsp
Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi..
Izod Impact, Notched 1.23 J/cm

@Temperature -40.0 °C
2.30 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Eastman Tenite 360E2R30016 Cellulose Acetate Propionate, Natural, Trsp
Applications:AppliancesPersonal Care and CosmeticsProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss..
Izod Impact, Notched 1.23 J/cm

@Temperature -40.0 °C
2.30 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Eastman Tenite 360E3V45516 Propionate Water Clear, Trsp
Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi..
Izod Impact, Notched 1.23 J/cm

@Temperature -40.0 °C
2.30 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Eastman Tenite 360E4861316 Cellulose Acetate Propionate, Clear, Trsp
Applications:ProfilesProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. T..
Izod Impact, Notched 1.23 J/cm

@Temperature -40.0 °C
2.30 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Eastman Tenite 485E3720023 Butyrate Clear, Trsp
Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi..
Izod Impact, Notched 1.23 J/cm

@Temperature 23.0 °C
2.30 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics LNP Verton PV007SV_YW8D151 PA 6
Preliminary data for 35% long fiber single pellet color filled PA6This data was supplied by SABIC-IP for the Americas region.