Mechanical Properties Metric English Comments
Izod Impact, Notched 0.560 J/cm

@Temperature 23.0 °C
1.05 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics Ultem 1110FV PEI
Enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant, NSF 51 listing.This data was supplied by SABIC-I..
Izod Impact, Notched 0.560 J/cm

@Temperature -30.0 °C
1.05 ft-lb/in

@Temperature -22.0 °F
ASTM D 256
SABIC Innovative Plastics Ultem 1110FV PEI
Enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant, NSF 51 listing.This data was supplied by SABIC-I..
Izod Impact, Notched 0.560 J/cm

@Temperature 23.0 °C
1.05 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics Ultem 1110V PEI
Enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card.This data was supplied by SABIC-IP for the Americas region.
Izod Impact, Notched 0.560 J/cm

@Temperature -30.0 °C
1.05 ft-lb/in

@Temperature -22.0 °F
ASTM D 256
SABIC Innovative Plastics Ultem 1110V PEI
Enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card.This data was supplied by SABIC-IP for the Americas region.
Izod Impact, Notched 0.560 J/cm

@Temperature 23.0 °C
1.05 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics Ultem 1110V PEI (Europe-Africa-Middle East)
Enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Izod Impact, Notched 0.560 J/cm

@Temperature -30.0 °C
1.05 ft-lb/in

@Temperature -22.0 °F
ASTM D 256
SABIC Innovative Plastics Ultem 1110V PEI (Europe-Africa-Middle East)
Enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Izod Impact, Notched 0.560 J/cm

@Temperature 23.0 °C
1.05 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics Ultem 1110V PEI (Asia Pacific)
Enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card.This data was supplied by SABIC-IP for the Asia Pacific region.
Izod Impact, Notched 0.560 J/cm

@Temperature -30.0 °C
1.05 ft-lb/in

@Temperature -22.0 °F
ASTM D 256
SABIC Innovative Plastics Ultem 1110V PEI (Asia Pacific)
Enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card.This data was supplied by SABIC-IP for the Asia Pacific region.
Izod Impact, Notched 0.560 J/cm

@Temperature 23.0 °C
1.05 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Eastman Eastar MN058 Copolyester
Eastar copolyesters are brilliantly clear polymers that have excellent impact strength, chemical resistance, dimensional stability, and low shrinkage rates. Eastar MN058 Copolyester is a medical gra..
Izod Impact, Notched 0.560 J/cm

@Temperature 23.0 °C
1.05 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Eastman Eastar MN059 Copolyester
Eastar copolyesters are brilliantly clear polymers that have excellent impact strength, chemical resistance, dimensional stability, and low shrinkage rates. Eastar MN059 Copolyester is a medical gra..
Izod Impact, Notched 0.560 J/cm

@Temperature 23.0 °C
1.05 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Eastman Eastar EN059 Copolyester, Natural
Applications:Cosmetics/personal care packagingDeodorant PackagingFragrance packagingOral hygienePlastics for hygiene feminine productsToothbrushesToys/Sporting goodsWriting instrumentsProduct Descri..
Izod Impact, Notched 0.560 J/cm

@Temperature 23.0 °C
1.05 ft-lb/in

@Temperature 73.4 °F
ASTM-D256
Braskem Prisma 3410 RACO Random Polypropylene Copolymer
Prisma 3410 is a medium melt flow rate random copolymer designed for injection molding. This product exhibits exceptional transparency, very good stiffness/impact strength balance, and excellent pro..