Polymer Property : Izod Impact, Notched = 0.940 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.940 J/cm

@Thickness 4.00 mm,
Temperature 23.0 °C
1.76 ft-lb/in

@Thickness 0.157 in,
Temperature 73.4 °F
ISO 180
Premix Thermoplastics PRE-ELEC® PP 1375
PRE-ELEC PP 1375 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELE..
Izod Impact, Notched 0.940 J/cm

@Temperature 23.0 °C
1.76 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Eastman Provista MP001 Copolymer
Provista Copolymer MP001 is a resin specifically developed for extrusion into profiles where aesthetics such as high clarity and gloss, coupled with design flexibility, drive demand. Compared to com..
Izod Impact, Notched 0.940 J/cm

@Temperature 23.0 °C
1.76 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Eastman Provista UVI Copolymer
Provista UVI is a Provista copolymer with an indoor/outdoor UV package added to prevent yellowing caused by light. Provista copolymer is a resin specifically developed for extrusion into profiles wh..
Izod Impact, Notched 0.940 J/cm

@Temperature 23.0 °C
1.76 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Eastman Provista UVO Copolymer
Provista UVO is a Provista copolymer with an indoor/outdoor UV package added to prevent yellowing caused by light. Provista copolymer is a resin specifically developed for extrusion into profiles wh..
Izod Impact, Notched 0.940 J/cm

@Temperature 23.0 °C
1.76 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Eastman Eastar GN046 Copolyester, Natural
Eastar Copolyester GN046 is a very high melt strength copolyester targeted for extrusion blow molding applications. Blow molding of large parts (up to several pounds) are possible with this material..