Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.677 J/cm @Thickness 6.35 mm |
1.27 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Starex® GR-4020L ABS, Glass Filled ABS/GF material that is used in printer LBP fuserInformation provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.677 J/cm @Thickness 6.35 mm |
1.27 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Starex® GR-4020L ABS, Glass Filled ABS/GF material that is used in printer LBP fuserInformation provided by Samsung Cheil Industries. |