Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.641 J/cm @Temperature -30.0 °C |
1.20 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
Noble Polymers Regis™ 225104 Thermoplastic Olefin (TPO) Regis is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. We have created Regis for use in bumpers and bumper fascias, air dams, exterior panels, materi.. |
|||
Izod Impact, Notched | 0.641 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
1.20 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D256 |
Techmer ES HiFill FR® PA6/6 GF30 FR-N 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightFeatures: Flame Retardant and Halogen FreeInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 0.641 J/cm @Temperature 0.000 °C |
1.20 ft-lb/in @Temperature 32.0 °F |
ASTM D256 |
Formosa Plastics Formolene® 2315N Impact Copolymer Polypropylene Impact Copolymer for Injection Molding Applications Requiring Stiffness Formolene® 2315N is a high flexural modulus copolymer of polypropylene designed and formulated for injection-molded applicati.. |
|||
Izod Impact, Notched | 0.641 J/cm @Temperature 23.0 °C |
1.20 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Formosa Plastics Formolene® 6335N Impact Copolymer Polypropylene Impact Copolymer - Designed to Meet the Physical Requirements of Automotive Interior Trim Formolene® 6335N is an engineered, medium impact copolymer polypropylene. It was specifically developed to.. |
|||
Izod Impact, Notched | 0.641 J/cm @Temperature -30.0 °C |
1.20 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
Formosa Plastics Formolene® 6575N Impact Copolymer Polypropylene Impact Copolymer for High Speed injection Molded Applications Formolene® 6575N is a very high melt flow, medium impact copolymer of polypropylene. It is designed for such applications as packaging,.. |
|||
Izod Impact, Notched | 0.641 J/cm @Temperature -18.0 °C |
1.20 ft-lb/in @Temperature -0.400 °F |
ASTM D256A |
Formosa Plastics Formolene® 6535N Impact Copolymer Polypropylene Impact Copolymer - Designed to Meet the Physical Requirements of Automotive Interior Trim Formolene® 6535N is an engineered, medium impact copolymer polypropylene. It was specifically developed to.. |
|||
Izod Impact, Notched | 0.641 J/cm @Thickness 3.17 mm, Temperature 0.000 °C |
1.20 ft-lb/in @Thickness 0.125 in, Temperature 32.0 °F |
ASTM D256 |
Diamond Polymers Centrex® 810 Injection Molding Grade Centrex 810 resin is a soft-flow, high-gloss, and medium-impact grade of ASA (acrylonitrile-styrene-acrylate). It is an injection molding grade with a good balance of physical properties, gloss and .. |
|||
Izod Impact, Notched | 0.641 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
1.20 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D-256 |
Axiall LR-5009 Rigid PVC, Molding, All Colors Georgia Gulf LR-5009 is an economical high flow rigid PVC fittings compound designed for multi-cavity molds and large diameter fittings. This compound is characterized by excellent process ability,.. |