Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Notched = 0.640 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.640 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
1.20 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Compression Molded, Across Flow; ASTM D256A
PolyOne Geon™ Vinyl Rigid Extrusion 87345 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Izod Impact, Notched 0.640 J/cm

@Thickness 3.18 mm,
Temperature -40.0 °C
1.20 ft-lb/in

@Thickness 0.125 in,
Temperature -40.0 °F
Compression Molded, Across Flow; ASTM D256A
PolyOne Geon™ Vinyl Rigid Extrusion L0676 Polyvinyl Chloride, Rigid (PVC, Rigid)
Note: NSF listings are obtained on specific colors. Contact PolyOne for the latest listing of approved colors for this product. Note: The Cell Classification was determined using the notched Izod te..
Izod Impact, Notched 0.640 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
1.20 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
PolyOne Geon™ Vinyl Fittings M1012 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Izod Impact, Notched 0.640 J/cm

@Temperature -40.0 °C
1.20 ft-lb/in

@Temperature -40.0 °F
Solvay Specialty Polymers Halar® 500 ECTFE Fluoropolymer  (discontinued **)
Data provided by the manufacturer.HALAR® Fluoropolymers have excellent barrier properties, high resistance to a variety of corrosive chemicals and solvents, low flammability, and ease of processing..
Izod Impact, Notched 0.640 J/cm

@Temperature 77.0 °C
1.20 ft-lb/in

@Temperature 171 °F
DAM; ASTM D256
DuPont Performance Polymers Zytel® 105F BK010 Nylon 66  (Unverified Data**)
Zytel® 105F BK010 is a lubricated, fast cycling, weather resistant PA 66 resin. Zytel® 105F BK010 contains finely dispersed carbon black.Information provided by DuPont Performance Polymers
Izod Impact, Notched 0.640 J/cm

@Thickness 3.20 mm,
Temperature -40.0 °C
1.20 ft-lb/in

@Thickness 0.126 in,
Temperature -40.0 °F
ASTM-D256
Ineos ABS Lustran® 433 ABS, General-Purpose Injection Molding Grade
Lustran® ABS 433 is a general-purpose injection molding grade of ABS (Acrylonitrile Butadiene Styrene). It is a high-impact, high-gloss ABS, available only in natural (000000) and black (904000)...
Izod Impact, Notched 0.640 J/cm

@Thickness 3.20 mm,
Temperature -40.0 °C
1.20 ft-lb/in

@Thickness 0.126 in,
Temperature -40.0 °F
ASTM-D256
Ineos ABS Lustran® 633 ABS, Injection Molding Grade
Lustran® ABS 633 is a general-purpose injection molding grade of ABS (Acrylonitrile Butadiene Styrene). It offers a good balance of physical properties, high gloss, and good moldability. Typical ..
Izod Impact, Notched 0.640 J/cm

@Thickness 3.17 mm
1.20 ft-lb/in

@Thickness 0.125 in
ASTM D256
LG Chemical MI-750 MIPS
Medium impact
Izod Impact, Notched 0.640 J/cm

@Temperature -30.0 °C
1.20 ft-lb/in

@Temperature -22.0 °F
3.2 mm (0.125 in) notch
Kraton® G1652 + PP blend + Talc (12/21/67)
Unmodified polypropylene has high rigidity and good heat resistance, but poor impact resistance, especially at low temperatures. Blending KRATON D and G polymers with PP significantly improves the ..
Izod Impact, Notched 0.640 J/cm

@Thickness 6.35 mm
1.20 ft-lb/in

@Thickness 0.250 in
ASTM D256
LG Chemical 401 AF Flame Retardant HIPS
NON-DECA, Flame retardant, Safety standards: listed with UL CSA, and classified according to IEC 707, Meet requirements for flammability, mechanical and electrical properties, uses non-bromide as fl..
Izod Impact, Notched 0.640 J/cm

@Temperature 23.0 °C
1.20 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics Ultem 2210K PEI (Europe-Africa-Middle East)
20% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Izod Impact, Notched 0.640 J/cm

@Temperature -30.0 °C
1.20 ft-lb/in

@Temperature -22.0 °F
ASTM D 256
SABIC Innovative Plastics Ultem 2210K PEI (Europe-Africa-Middle East)
20% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Izod Impact, Notched 0.640 J/cm

@Temperature 23.0 °C
1.20 ft-lb/in

@Temperature 73.4 °F
Compression Molded; ASTM D256
Styron STYRONâ„¢ 6500 Ignition Resistant Polystyrene Resin
Overview: STYRONâ„¢ 6500 is an ignition-resistant polystyrene resin with excellent balance of strength, heat resistance and flow properties that are tailor-made for consumer electronics applicati..
Izod Impact, Notched 0.640 J/cm

@Temperature -30.0 °C
1.20 ft-lb/in

@Temperature -22.0 °F
ASTM D 256
SABIC Innovative Plastics Noryl PPX PPX615 PPE+PP
Good chemical resistance. Designed for a balance of stiffness and practical impact strength.This data was supplied by SABIC-IP for the Americas region.
Izod Impact, Notched 0.640 J/cm

@Temperature -30.0 °C
1.20 ft-lb/in

@Temperature -22.0 °F
ASTM D 256
SABIC Innovative Plastics Noryl PPX PPX615 PPE+PP (Asia Pacific)
Good chemical resistance. Designed for a balance of stiffness and practical impact strength.This data was supplied by SABIC-IP for the Asia Pacific region.
Izod Impact, Notched 0.640 J/cm

@Temperature -30.0 °C
1.20 ft-lb/in

@Temperature -22.0 °F
ASTM D 256
SABIC Innovative Plastics Noryl PPX PPX615 PPE+PP (Europe-Africa-Middle East)
Good chemical resistance. Designed for a balance of stiffness and practical impact strength.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Izod Impact, Notched 0.640 J/cm

@Temperature 23.0 °C
1.20 ft-lb/in

@Temperature 73.4 °F
Absolute Drying; ASTM-D256
Toyobo GLAMIDE® T-400G15 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Izod Impact, Notched 0.640 J/cm

@Temperature -40.0 °C
1.20 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Lubrizol Estaloc® 61225 Polyester-Type Thermoplastic Alloy
Type: Estaloc® 61225 Alloy RETPU is a polyester-type thermoplastic alloy.Features: Fast cycling, dimensional stability, durability, aesthetics, low temperature impact.Uses: Injection molding.Availa..
Izod Impact, Notched 0.640 J/cm

@Temperature -40.0 °C
1.20 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Eastman Eastar MN004 Copolyester
Eastar Copolyesters are brilliantly clear polymers that have excellent impact strength, chemical resistance, dimensional stability, and low shrinkage rates. Eastar MN004 contains a mold release.Appl..
Izod Impact, Notched 0.640 J/cm

@Thickness 3.17 mm,
Temperature -18.0 °C
1.20 ft-lb/in

@Thickness 0.125 in,
Temperature -0.400 °F
ASTM D256
Diamond Polymers Centrex® 485 Sheet Extrusion Grade
Centrex 485 resin is a low-gloss, medium-impact grade of ASA (acrylonitrile-styrene-acrylate) with good resistance to weather aging. It has good melt strength for extrusion and thermoforming, and it..
Copyright © lookpolymers.com All Rights Reserved