Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.600 J/cm @Temperature 23.0 °C |
1.12 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
SABIC PP 49MK40 Polypropylene Impact Copolymer for Injection Molding Product Description: PP 49MK40 is a high crystalline impact copolymer with high stiffness. This grade is especially developed for producing injection molded articles. The grade contains an antist.. |
|||
Izod Impact, Notched | 0.600 J/cm @Temperature -30.0 °C |
1.12 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycolac® MG8000SR ABS This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 0.600 J/cm @Temperature -30.0 °C |
1.12 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycolac® MG8000SR ABS (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 0.600 J/cm @Temperature -30.0 °C |
1.12 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycolac® MG8000SR ABS (Europe-Africa-Middle East) This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Notched | 0.600 J/cm @Thickness 4.00 mm, Temperature 23.0 °C |
1.12 ft-lb/in @Thickness 0.157 in, Temperature 73.4 °F |
ISO 180 |
Premix Thermoplastics PRE-ELEC® PS 1328 PRE-ELEC PS 1328 is a conductive thermoplastic compound based on polystyrene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC .. |
|||
Izod Impact, Notched | >= 0.600 J/cm @Temperature -20.0 °C |
>= 1.12 ft-lb/in @Temperature -4.00 °F |
ASTM D256 |
NIZHNEKAMSKNEFTEKHIM PP 8332C (EPD60R) Propylene and Ethylene Block Polymer Product obtained by copolymerization of propylene with ethylene in presence of complex metalorganic catalysts. It incorporates increased long-term thermal stability, thermal-oxidative degradation r.. |
|||
Izod Impact, Notched | 0.600 J/cm @Temperature -30.0 °C |
1.12 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Ultem UR9076LG PEI Standard flow mineral filled Polyetherimide Blend. Restricted sales to GE Specialty Film & Sheet.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 0.600 J/cm @Temperature -30.0 °C |
1.12 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Xenoy® 6380U PBT+PET (Asia Pacific) XENOY 6380U is a 30% glass reinforced, UV stabilized grade, that combines high stiffness with improved ductility. The combination of mechanical properties at high and low temperatures and chemical r.. |
|||
Izod Impact, Notched | 0.600 J/cm @Temperature 23.0 °C |
1.12 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Noryl GTX GTX966 PPE+PA66 >PPE+PA66-I-TD10 |
|||
Izod Impact, Notched | 0.600 J/cm @Temperature -30.0 °C |
1.12 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Noryl GTX GTX966 PPE+PA66 >PPE+PA66-I-TD10 |
|||
Izod Impact, Notched | 0.600 J/cm @Temperature -30.0 °C |
1.12 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Noryl GTX GTX966 PPE+PA66 (Europe-Africa-Middle East) >PPE+PA66-I-TD10 |
|||
Izod Impact, Notched | 0.600 J/cm @Temperature -30.0 °C |
1.12 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Xenoy® X5630 PC+PET Mineral filled PC/PET blend with high heat dimensional stability, low shrinkage and low CTE, especially for painted applicationsThis data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 0.600 J/cm @Temperature 23.0 °C |
1.12 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Toyobo GLAMIDE® T-714E Transparent Nylon GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Izod Impact, Notched | 0.600 J/cm @Temperature 23.0 °C |
1.12 ft-lb/in @Temperature 73.4 °F |
Practical Use (Water Absorption 1.9%); ASTM-D256 |
Toyobo GLAMIDE® TY-502NZ 6T-Nylon GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Izod Impact, Notched | 0.600 J/cm @Temperature -40.0 °C |
1.12 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Toyobo NB-5620S Nylon/Olefin Alloy, 15% Mineral Reinforced (Conditioned) Features: 15% Mineral Reinforced, Light WeightInformation provided by Toyobo. |
|||
Izod Impact, Notched | 0.600 J/cm @Temperature -40.0 °C |
1.12 ft-lb/in @Temperature -40.0 °F |
Practical Use (Water Absorption 2.4%); ASTM-D256 |
Toyobo GLAMIDE® NB-1700 Nylon/Olefin GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Izod Impact, Notched | 0.600 J/cm @Temperature -40.0 °C |
1.12 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Eastman DuraStar DS2000 Polymer, Natural Durastar DS2000 polymer has excellent appearance and is nearly water-clear. Its most outstanding features are toughness, chemical resistance, and excellent processing characteristics. DS2000 has ver.. |
|||
Izod Impact, Notched | 0.600 J/cm @Temperature -40.0 °C |
1.12 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Eastman DuraStar DS2110UVI Polymer, Natural Durastar DS2110UVI polymer, contains an ultraviolet light stabilization package. It is recommended for indoor applications requiring enhanced color stability upon extended exposure to fluorescent li.. |
|||
Izod Impact, Notched | 0.600 J/cm @Temperature -40.0 °C |
1.12 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Eastman DuraStar MN620 Polymer, Natural Applications:Blood therapyDrug deliveryIV componentsMedicalSurgical instrumentsKey Attributes:Chemical resistance to most medical solvents including lipids and IPAProduct Description: DuraStar Poly.. |
|||
Izod Impact, Notched | 0.600 J/cm @Temperature -40.0 °C |
1.12 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Eastman Eastar BR203 Copolyester Eastar BR203 Copolyester contains a mold release additive. It has excellent appearance and is nearly water-clear. Its most outstanding features are its chemical resistance and processing capabilitie.. |
|||
Izod Impact, Notched | 0.600 J/cm @Temperature 0.000 °C |
1.12 ft-lb/in @Temperature 32.0 °F |
ASTM D 638 |
Cossa Polimeri ESTADIENE 0460 GF Acrylonitrile Butadiene Styrene, 30% Glass Filled ABS with 30% glass fiber reinforcementExcellent dimensional stability, low shrinkage, good impact resistanceInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 0.600 J/cm @Temperature 23.0 °C |
1.12 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
Cossa Polimeri ESTAPROP 1000 V2 K Flame Retardant Polypropylene PP copolymerFlame retardant class V2, PBDE free, good processability, good impact strengthInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 0.600 J/cm @Temperature 23.0 °C |
1.12 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
Cossa Polimeri ESTAPROP 1006 V2 K Flame Retardant Polypropylene PP copolymerFlame retardant class V2, PBDE and antimony trioxide free, no blooming, low smoke emission, good physical and mechanical characteristicsInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 0.600 J/cm @Temperature 23.0 °C |
1.12 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
Cossa Polimeri ESTAPROP H 0560 GF Polypropylene, 30% Glass Filled PP homopolymer 30% glass fiber reinforcedGood physical and mechanical characteristicsInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 0.600 J/cm @Thickness 3.20 mm, Temperature -30.0 °C |
1.12 ft-lb/in @Thickness 0.126 in, Temperature -22.0 °F |
ASTM D256, ISO 180/4a |
EPICHEM Epilac ABS Acrylonitrile Butadiene Styrene |
|||
Izod Impact, Notched | 0.600 J/cm @Thickness 3.20 mm, Temperature -40.0 °C |
1.12 ft-lb/in @Thickness 0.126 in, Temperature -40.0 °F |
ASTM D256, ISO 180/4a |
EPICHEM Epilon G4-PC 20% GF Polycarbonate, 20% Glass Fiber Characteristics: 20% glass fibre filled, excellent mechanical properties |
|||
Izod Impact, Notched | 0.600 J/cm @Temperature 0.000 °C |
1.12 ft-lb/in @Temperature 32.0 °F |
ASTM D 638 |
Cossa Polimeri ESTASTIR HI 1012 Polystyrene General purpose polystyreneHigh impact resistance, good melt flow rate, good flexibilityInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 0.600 J/cm @Thickness 3.20 mm, Temperature -30.0 °C |
1.12 ft-lb/in @Thickness 0.126 in, Temperature -22.0 °F |
ASTM D256, ISO 180/4a |
EPICHEM Epiryl G2 PPO 20GF Polyphenylene oxide, 20% Glass Fiber Characteristics: 20% glass fibre filled |
|||
Izod Impact, Notched | 0.600 J/cm @Temperature -20.0 °C |
1.12 ft-lb/in @Temperature -4.00 °F |
ASTM D256A |
Braskem CP 195 Injection Molding Polypropylene Description: CP 195 is a very high melt flow rate heterophasic copolymer developed for high speed injection moulding machines and high productivity thin-walled injection moulded parts. The product f.. |
|||
Izod Impact, Notched | 0.600 J/cm @Temperature -20.0 °C |
1.12 ft-lb/in @Temperature -4.00 °F |
ASTM D256 |
Carmel Olefins CAPILENE® SE 50 E Polypropylene Impact Copolymer Description: CAPILENE® SE 50 E is a low melt flow rate impact copolymer intended for sheet extrusion. It exhibits excellent impact strength even at low temperatures, combined with good processabi.. |