Polymer Property : Izod Impact, Notched = 0.480 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.480 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
0.899 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Compression Molded, Flow; ASTM D256A
PolyOne Geon™ Vinyl Rigid Extrusion 78761 Polyvinyl Chloride, Rigid (PVC, Rigid)
Note: NSF listings are obtained on specific colors. Contact PolyOne for the latest listing of approved colors for this product.Information provided by PolyOne
Izod Impact, Notched 0.480 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
0.899 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Compression Molded, Across Flow; ASTM D256A
PolyOne Geon™ Vinyl Rigid Extrusion L8761 Polyvinyl Chloride, Rigid (PVC, Rigid)
Note: NSF listings are obtained on specific colors. Contact PolyOne for the latest listing of approved colors for this product.Information provided by PolyOne
Izod Impact, Notched 0.480 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
0.899 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Compression Molded, Flow; ASTM D256A
PolyOne Geon™ Vinyl Rigid Extrusion L8761 Polyvinyl Chloride, Rigid (PVC, Rigid)
Note: NSF listings are obtained on specific colors. Contact PolyOne for the latest listing of approved colors for this product.Information provided by PolyOne
Izod Impact, Notched 0.480 J/cm

@Temperature 23.0 °C
0.899 ft-lb/in

@Temperature 73.4 °F
ASTM D256
DuPont Performance Polymers Crastin® 6130 NC010 PBT  (Unverified Data**)
Crastin® 6130 NC010 is an unreinforced, medium high viscosity polybutylene terephthalate resin for extrusion and injection molding.Information provided by DuPont Performance Polymers
Izod Impact, Notched 0.480 J/cm

@Temperature 23.0 °C
0.899 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Eastman Eastar GN102 Copolyester  (discontinued **)
Eastar GN102 copolyester is a glycol modified polyethylene terephthalate (PET) that contains an ultraviolet inhibitor and mold release. Eastar GN102 copolyester will not crystallize and thus offers ..
Izod Impact, Notched 0.480 J/cm

@Temperature -30.0 °C
0.899 ft-lb/in

@Temperature -22.0 °F
injection molded specimen; ASTM D256
Phillips Sumika Marlex® AGM-110 Reactor Thermoplastic Polyolefins, Cold Temperature Impact Resistant  (discont
Applications: Automotive fascias and claddingsConsumer productsTotes and binsInformation provided by Chevron Phillips.Phillips Sumika Polypropylene Company has been shut down, as announced in 2011. ..
Izod Impact, Notched 0.480 J/cm

@Temperature 23.0 °C
0.899 ft-lb/in

@Temperature 73.4 °F
DAM; ASTM D256
DuPont Performance Polymers Zytel® 105F BK010 Nylon 66  (Unverified Data**)
Zytel® 105F BK010 is a lubricated, fast cycling, weather resistant PA 66 resin. Zytel® 105F BK010 contains finely dispersed carbon black.Information provided by DuPont Performance Polymers
Izod Impact, Notched 0.480 J/cm

@Temperature -40.0 °C
0.899 ft-lb/in

@Temperature -40.0 °F
DAM; ASTM D256
DuPont Performance Polymers Zytel® 7304 NC010 Nylon 6  (Unverified Data**)
Zytel® 7304 NC010 is a medium viscosity, unlubricated polyamide 6 resin for extrusion applications.Information provided by DuPont Performance Polymers
Izod Impact, Notched 0.480 J/cm

@Temperature 23.0 °C
0.899 ft-lb/in

@Temperature 73.4 °F
50%RH; ASTM D256
DuPont Performance Polymers Zytel® 157HSL BK010 Nylon 612  (Unverified Data**)
Zytel® 157HSL BK010 is a heat stabilized, weatherable, lubricated polyamide 612 resin that is suitable for molding and extrusion applications.Information provided by DuPont Performance Polymers
Izod Impact, Notched 0.480 J/cm

@Temperature -40.0 °C
0.899 ft-lb/in

@Temperature -40.0 °F
DAM; ASTM D256
DuPont Performance Polymers Zytel® 158L NC010 Nylon 612  (Unverified Data**)
Zytel® 158L NC010 is an intermediate viscosity, lubricated polyamide 612 resin that is suitable for molding and extrusion applications.Information provided by DuPont Performance Polymers
Izod Impact, Notched 0.480 J/cm

@Thickness 3.20 mm,
Temperature -40.0 °C
0.899 ft-lb/in

@Thickness 0.126 in,
Temperature -40.0 °F
ASTM-D256
Ineos ABS Lustran® 256 Extrusion Blending Grade
Lustran® ABS 256 resin is a natural, medium-flow, medium-impact, low-gloss, low-gel extrusion grade of ABS (Acrylonitrile Butadiene Styrene). It is used for blending with other Lustran® ABS vi..
Izod Impact, Notched 0.480 J/cm

@Thickness 3.20 mm,
Temperature -40.0 °C
0.899 ft-lb/in

@Thickness 0.126 in,
Temperature -40.0 °F
ASTM-D256
Ineos ABS Lustran® ABS 248FC Medical & Food Contact Grade
Lustran® ABS 248FC resin is a high-gloss, medium-impact grade of ABS (acrylonitrile butadiene styrene). This injection molding grade offers a good balance of physical properties and has been desi..
Izod Impact, Notched 0.480 J/cm

@Temperature 23.0 °C
0.899 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics Ultem HFATX200 PEI+PCE
High flow Polyetherimide blend with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Americas region.
Izod Impact, Notched 0.480 J/cm

@Temperature 23.0 °C
0.899 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics Ultem HFATX200 PEI+PCE (Asia Pacific)
High flow Polyetherimide blend with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Asia Pacific region.
Izod Impact, Notched 0.480 J/cm

@Temperature 23.0 °C
0.899 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics Ultem HFATX200 PEI+PCE (Europe-Africa-Middle East)
High flow Polyetherimide blend with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Izod Impact, Notched 0.480 J/cm

@Temperature -40.0 °C
0.899 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Eastman Tenite 105E3V36327 Acetate Clear, Trsp
Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi..
Izod Impact, Notched 0.480 J/cm

@Temperature -20.0 °C
0.899 ft-lb/in

@Temperature -4.00 °F
ASTM D256A
Dow C759-21NA Polypropylene Impact Copolymer Resin
DOW C759-21NA Polypropylene Resin is an impact copolymer designed for injection molding with high stiffness, good impact resistance, and good antistatic properties. Key applications include foldabl..
Izod Impact, Notched 0.480 J/cm

@Temperature 23.0 °C
0.899 ft-lb/in

@Temperature 73.4 °F
ASTM D256A
Dow H349-02 Polypropylene Homopolymer Resin
H349-02 Polypropylene Resin intended for use in biaxial oriented (BOPP) film processes. This product can also be used in extrusion and thermoforming applications where improved melt strength is des..
Izod Impact, Notched 0.480 J/cm

@Temperature -40.0 °C
0.899 ft-lb/in

@Temperature -40.0 °F
ASTM D256
BASF Ultramid® 8270 HS BK 102 PA6 (Conditioned)
Description: Ultramid 8270 HS BK-102 is a thermally modified pigmented black, PA6 blow molding compound exhibiting exceptional toughness and melt strength ideally suited for blow molding, profile ex..
Izod Impact, Notched 0.480 J/cm

@Temperature -30.0 °C
0.899 ft-lb/in

@Temperature -22.0 °F
injection molded specimen; ASTM D256
Phillips Sumika Marlex® ABF-110 Reactor Thermoplastic Polyolefin, Cold Temperature Impact Resistant  (disconti
Applications: Automotive fascias and claddingsConsumer productsTotes and binsInformation provided by Chevron Phillips.Phillips Sumika Polypropylene Company has been shut down, as announced in 2011. ..