Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.427 J/cm @Temperature -20.0 °C |
0.800 ft-lb/in @Temperature -4.00 °F |
1/8'' notched bar; ASTM D256 |
Ineos L12N-00 Polypropylene Impact Copolymer This is a medium melt flow rate, nucleated impact copolymer polypropylene for injection molding and compounding applications. This material meets the requirements of the U.S. Food and Drug Administ.. |
|||
Izod Impact, Notched | 0.427 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
0.800 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D256 |
Techmer ES HiFill® PA6 GF/M25 HS L BK 25% Glass/Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral, 25% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and LubricatedAppearance: BlackTPCI.. |
|||
Izod Impact, Notched | 0.427 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
0.800 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D256 |
Techmer ES HiFill® PA6 GF/M30 HS BK 10/20% Glass/Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by Weight and Mineral, 20% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat .. |
|||
Izod Impact, Notched | 0.427 J/cm @Thickness 3.17 mm, Temperature -30.0 °C |
0.800 ft-lb/in @Thickness 0.125 in, Temperature -22.0 °F |
ASTM D256 |
Diamond Polymers Centrex® 835 Sheet Extrusion Grade Centrex 835 resin is a low-gloss grade of ASA (acrylonitrile-styrene-acrylate) with good resistance to weather aging. It has good melt strength for extrusion and thermoforming applications. Centrex .. |
|||
Izod Impact, Notched | 0.427 J/cm @Thickness 3.17 mm, Temperature -30.0 °C |
0.800 ft-lb/in @Thickness 0.125 in, Temperature -22.0 °F |
ASTM D256 |
Diamond Polymers DIAMALOY GLY 7510 High Heat ASA Weatherable Polymer Diamaloy GLY 7510 resin is a high gloss, high heat and high impact grade of ASA (acrylonitrile-styrene-acrylate) with good resistance to weather aging. This product is rated f1 by UL and be customed.. |
|||
Izod Impact, Notched | 0.427 J/cm @Thickness 6.35 mm, Temperature 23.0 °C |
0.800 ft-lb/in @Thickness 0.250 in, Temperature 73.4 °F |
ASTM D-256 |
Axiall 5009 Rigid PVC, Molding Georgia Gulf 5009 is a type I, Grade I rigid vinyl injection molding compound designed for fittings and parts of similar confiation where maximum tensile strength and/or chemical resistance is requi.. |
|||
Izod Impact, Notched | 0.427 J/cm @Temperature -30.0 °C |
0.800 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
Formosa Plastics Formolene® 6620A Impact Copolymer Polypropylene High Impact Copolymer for Injection Molding Formolene® 6620A is a copolymer of polypropylene designed and formulated for injection molding applications including pails, crates and furniture. It con.. |
|||
Izod Impact, Notched | 0.427 J/cm @Temperature -30.0 °C |
0.800 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
Formosa Plastics Formolene® 6630A Impact Copolymer Polypropylene Impact Copolymer for Injection Molding Applications Formolene® 6630A is a high impact copolymer of polypropylene designed and formulated for injection-molded applications. It contains a unique comb.. |
|||
Izod Impact, Notched | 0.427 J/cm @Thickness 3.17 mm, Temperature -17.8 °C |
0.800 ft-lb/in @Thickness 0.125 in, Temperature 0.000 °F |
ASTM D256 |
Styron INSPIRE™ TF3800 Polypropylene Information provided by DowThe Inspire brand was spun off from Dow Chemical to Styron in 2010 |