Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.380 J/cm @Temperature -20.0 °C |
0.712 ft-lb/in @Temperature -4.00 °F |
ASTM D256 |
SABIC PP 49MK40 Polypropylene Impact Copolymer for Injection Molding Product Description: PP 49MK40 is a high crystalline impact copolymer with high stiffness. This grade is especially developed for producing injection molded articles. The grade contains an antist.. |
|||
Izod Impact, Notched | 0.380 J/cm @Temperature -40.0 °C |
0.712 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
LATI LATISTAT 43/7-02 Low Density Polyethylene (LDPE) Base Conductive Plastic
(discontinued **) Description: Latistat materials have low specific resistivity. They feature partial electrical conductivity. Selected functional additives give materials with low specific resistivity and reasonable.. |
|||
Izod Impact, Notched | 0.380 J/cm @Temperature -20.0 °C |
0.712 ft-lb/in @Temperature -4.00 °F |
ASTM D256 |
LATI LATAN 13 K/30 30% Carbon Fiber Reinforced Polyoxymethylene Copolymer (POM)
(Unverified Data**) Description: Latan series thermoplastics are polyoxymethylene copolymer (POM) products. The main applications for Latan feature good wear resistance, chemical inertness and low water absorption (gea.. |
|||
Izod Impact, Notched | 0.380 J/cm @Temperature 23.0 °C |
0.712 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LATI LATAN 13 K/30 30% Carbon Fiber Reinforced Polyoxymethylene Copolymer (POM)
(Unverified Data**) Description: Latan series thermoplastics are polyoxymethylene copolymer (POM) products. The main applications for Latan feature good wear resistance, chemical inertness and low water absorption (gea.. |
|||
Izod Impact, Notched | 0.380 J/cm @Temperature -30.0 °C |
0.712 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Ultem DT1800E PEI Blend Improved ductility, transparent, standard flow Polyetherimide blend (Tg 200C) with internal mold release and enhanced ductility. ECO Conforming.This data was supplied by SABIC-IP for the Americas re.. |
|||
Izod Impact, Notched | 0.380 J/cm @Temperature -30.0 °C |
0.712 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Ultem DT1800E PEI Blend (Asia Pacific) Improved ductility, transparent, standard flow Polyetherimide blend (Tg 200C) with internal mold release and enhanced ductility. ECO Conforming.This data was supplied by SABIC-IP for the Asia Pacifi.. |
|||
Izod Impact, Notched | 0.380 J/cm @Temperature -30.0 °C |
0.712 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Ultem DT1800E PEI Blend (Europe-Africa-Middle East) Improved ductility, transparent, standard flow Polyetherimide blend (Tg 200C) with internal mold release and enhanced ductility. ECO Conforming.This data was supplied by SABIC-IP for the Europe-Afri.. |
|||
Izod Impact, Notched | 0.380 J/cm @Temperature -40.0 °C |
0.712 ft-lb/in @Temperature -40.0 °F |
Absolute Drying; ASTM-D256 |
Toyobo GLAMIDE® NB-5550 Nylon/Olefin GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Izod Impact, Notched | 0.380 J/cm @Temperature -40.0 °C |
0.712 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Eastman Eastar CN005 Copolyester, High Flow Grade Applications:CompactsCosmetic jar capsCosmetic jarsCosmetics/personal care packagingFragrance capsFragrance packagingLip gloss containersLipstick containersPersonal care bottlesKey Attributes:Abilit.. |
|||
Izod Impact, Notched | 0.380 J/cm @Temperature -40.0 °C |
0.712 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Eastman Eastar CN015 Copolyester, High Flow Grade with Mold Release Applications:CompactsCosmetic jar capsCosmetic jarsCosmetics/personal care packagingFragrance capsFragrance packagingLip gloss containersLipstick containersPersonal care bottlesKey Attributes:Abilit.. |
|||
Izod Impact, Notched | 0.380 J/cm @Temperature 23.0 °C |
0.712 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Braskem Prisma 2400 RACO Random Polypropylene Copolymer Prisma 2400 is a high melt flow rate random copolymer. This product is designed for the ISBM (Injection Stretch Blow Molding) process and offers low taste/odor. It can also be used in the blow moldi.. |
|||
Izod Impact, Notched | 0.380 J/cm @Temperature -20.0 °C |
0.712 ft-lb/in @Temperature -4.00 °F |
ASTM D256A |
Braskem CP 405 XP Injection Molding Polypropylene Applications: Caps for soft drinks. Information provided by Braskem |
|||
Izod Impact, Notched | 0.380 J/cm @Temperature -20.0 °C |
0.712 ft-lb/in @Temperature -4.00 °F |
ASTM D256 |
Braskem CP 405XP Compression Molding Polypropylene Heterophasic Copolymer Bottle caps for carbonated beverages.Information provided by Braskem. |