Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.353 J/cm @Thickness 6.35 mm |
0.661 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Infino® GP-5150GT PBT, 15% Glass Filled Low warpage with 15% GF reinforcement and can be used in the switches for microwave or ovensInformation provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.353 J/cm @Thickness 6.35 mm |
0.661 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Infino® GP-5150GT PBT, 15% Glass Filled Low warpage with 15% GF reinforcement and can be used in the switches for microwave or ovensInformation provided by Samsung Cheil Industries. |