Mechanical Properties Metric English Comments
Izod Impact, Notched 0.340 J/cm

@Temperature -30.0 °C
0.637 ft-lb/in

@Temperature -22.0 °F
ASTM D 256
SABIC Innovative Plastics Geloy EXGY30CP ASA
Pearlescent GELOY ASA resin with copper-look for capstock extrusion. Outstanding weatherability.This data was supplied by SABIC-IP for the Americas region.
Izod Impact, Notched 0.340 J/cm

@Temperature -30.0 °C
0.637 ft-lb/in

@Temperature -22.0 °F
ASTM D 256
SABIC Innovative Plastics Geloy FXTW30PE ASA
Pearlescent GELOY ASA resin with copper-look for capstock extrusion. Outstanding weatherability.This data was supplied by SABIC-IP for the Americas region.
Izod Impact, Notched 0.340 J/cm

@Temperature -40.0 °C
0.637 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Eastman 9921P PET Injection Molded  (discontinued **)
Voridian PET 9921P is produced at Voridian’s manufacturing sites in Rotterdam and Zarate, it is PTA/CHDM based, and it is sold to customers in the Europe, Middle East and Africa, Argentina, Bolivia..
Izod Impact, Notched 0.340 J/cm

@Temperature -30.0 °C
0.637 ft-lb/in

@Temperature -22.0 °F
ASTM D 256
SABIC Innovative Plastics Geloy FXTW30CP ASA
Pearlescent GELOY ASA resin with copper-look for capstock extrusion. Outstanding weatherability.This data was supplied by SABIC-IP for the Americas region.
Izod Impact, Notched 0.340 J/cm

@Temperature 23.0 °C
0.637 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics Noryl GTX APS8740 PPE+PPS
Noryl* APS8740 resin is a glass filled, high performance blend of PPE/PPS that exhibits an excellent balance of high-heat resistance, strength, flame retardant, and conductivity. This grade can be e..
Izod Impact, Notched 0.340 J/cm

@Temperature 23.0 °C
0.637 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics Noryl GTX APS8740 PPE+PPS (Asia Pacific)
Noryl* APS8740 resin is a glass filled, high performance blend of PPE/PPS that exhibits an excellent balance of high-heat resistance, strength, flame retardant, and conductivity. This grade can be e..
Izod Impact, Notched 0.340 J/cm

@Temperature 23.0 °C
0.637 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics Noryl GTX APS8740 PPE+PPS (Europe-Africa-Middle East)
Noryl* APS8740 resin is a glass filled, high performance blend of PPE/PPS that exhibits an excellent balance of high-heat resistance, strength, flame retardant, and conductivity. This grade can be e..
Izod Impact, Notched 0.340 J/cm

@Temperature -30.0 °C
0.637 ft-lb/in

@Temperature -22.0 °F
ASTM D256
Eastman TiGlaze SV Copolyester
TiGLAZE SV copolyester is a specialty copolyester for the architectural glazing industry, designed to provide a unique balance of toughness, stiffness and material value. The material has a CC1 Ligh..
Izod Impact, Notched 0.340 J/cm

@Temperature -20.0 °C
0.637 ft-lb/in

@Temperature -4.00 °F
ASTM D256A
Braskem CP 144 Coating Polypropylene
Information provided by Braskem
Izod Impact, Notched 0.340 J/cm

@Temperature 23.0 °C
0.637 ft-lb/in

@Temperature 73.4 °F
ASTM D256
DuPont Performance Polymers Delrin® 577 BK000 Acetal Homopolymer  (Unverified Data**)
Delrin® 577 BK000 is a medium viscosity acetal homopolymer containing 20% glass fiber filler, with high stiffness, low warpage and low creep for superior performance at elevated temperature. It con..