Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.214 J/cm @Temperature 0.000 °C |
0.400 ft-lb/in @Temperature 32.0 °F |
ASTM D256 |
Formosa Plastics Formolene® 3320B Random Copolymer Polypropylene Random Copolymer for Storage Boxes, Pill Vials and Containers Formolene® 3320B is a high flow random copolymer with fast cycle time and easy mold release. It is designed for injection molding appli.. |
|||
Izod Impact, Notched | 0.214 J/cm @Temperature 0.000 °C |
0.401 ft-lb/in @Temperature 32.0 °F |
ASTM D256A |
Dow H349-02 Polypropylene Homopolymer Resin H349-02 Polypropylene Resin intended for use in biaxial oriented (BOPP) film processes. This product can also be used in extrusion and thermoforming applications where improved melt strength is des.. |
|||
Izod Impact, Notched | 0.214 J/cm @Thickness 3.17 mm, Temperature -28.9 °C |
0.400 ft-lb/in @Thickness 0.125 in, Temperature -20.0 °F |
ASTM D256 |
Styron INSPIRE™ TF3800 Polypropylene Information provided by DowThe Inspire brand was spun off from Dow Chemical to Styron in 2010 |
|||
Izod Impact, Notched | 0.214 J/cm @Temperature 0.000 °C |
0.401 ft-lb/in @Temperature 32.0 °F |
ASTM D256A |
Braskem INSPIRE™ 222 Performance Polypropylene Polymer INSPIRE™ 222 Performance Polymer is intended for use in extrusion and thermoforming processes. It is especially suited in applications requiring excellent clarity and good stiffness.Contains a nuc.. |