Polymer Property : Hot Tack Strength = 2000 g/25 mm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Hot Tack Strength <= 2000 g/25 mm
<= 2000 g/in
Varies with seal bar temp.; Packforsk Method
DuPont™ Surlyn® 1652-1 Zinc Ionomer Resin for Blown/Cast Film and Extrusion Coating  (discontinued **)
Surlyn® 1652-1 is an ionomer resin available for use in blown/cast film and extrusion coating operations. It can be used in both extrusion and coextrusion equipment designed to process polyethylen..
Hot Tack Strength <= 2000 g/25 mm
<= 2000 g/in
Varies with seal bar temp.; Packforsk Method
DuPont™ Surlyn® 1702-1 Zinc Ionomer Resin for Extrusion Coating  (discontinued **)
Surlyn® 1702-1 is an ionomer resin available for use in conventional extrusion coating and coextrusion coating equipment designed to process polyethylene resins. Applications: Medical/pharmaceutic..
Hot Tack Strength 2000 g/25 mm
2000 g/in
Seal Bar Temp approx. 115-145°C; Packforsk Method
DuPont™ Surlyn® 1601 Sodium Ionomer Resin for Blown and Cast Film
Surlyn® 1601 is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Applications: Meat, poultry, sea..
Hot Tack Strength 2000 g/25 mm
2000 g/in
Seal Bar Temp approx. 120-145°C; Packforsk Method
DuPont™ Surlyn® 1601-2 Sodium Ionomer Resin for Blown and Cast Film
Surlyn® 1601-2 is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Applications: Meat, poultry, s..
Hot Tack Strength 2000 g/25 mm
2000 g/in
Seal Bar Temp approx. 110-150°C; Packforsk Method
DuPont™ Surlyn® 1601-2LM Sodium Ionomer Resin for Blown and Cast Film
Surlyn® 1601-2LM (Low Moisture) is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Applications:..
Hot Tack Strength <= 2000 g/25 mm
<= 2000 g/in
Varies with seal bar temp.; Packforsk Method
DuPont™ Surlyn® 1652 Zinc Ionomer Resin for Flexible Packaging
Surlyn® 1652 is an ionomer resin available for use in blown/cast film and extrusion coating operations. It can be used in both extrusion and coextrusion equipment designed to process polyethylene ..
Hot Tack Strength <= 2000 g/25 mm
<= 2000 g/in
Varies with seal bar temp.; Packforsk Method
DuPont™ Surlyn® 1857 Zinc Ionomer Resin for Blown and Cast Film
Surlyn® 1857 is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Applications: Meat, poultry, sea..
Hot Tack Strength <= 2000 g/25 mm
<= 2000 g/in
Varies with seal bar temp.; Packforsk Method
DuPont™ Surlyn® 1702 Zinc Ionomer Resin for Extrusion Coating
Surlyn® 1702 is an ionomer resin available for use in conventional extrusion coating and coextrusion coating equipment designed to process polyethylene resins. Applications: Medical/pharmaceutical..
Hot Tack Strength 2000 g/25 mm
2000 g/in
seal bar 105°C; Packforsk method.
DuPont Nucrel® 1207 Ethylene-Methacrylic Acid Copolymer Resin for Extrusion Coating/Laminating  (discontinued
12 wt% Methacrylic Acid.Nucrel® 1207 is an ethylene-methacrylic acid copolymer resin available for use in conventional extrusion coating, coextrusion coating, and extrusion laminating equipment des..