Polymer Property : Impact Test = 95.0 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Impact Test 95.0 J
70.1 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics Lexan® HFD1830 PC Copolymer
40 MFR LEXAN High Flow Ductile Copolymer UV Stabilized
Impact Test 95.0 J
70.1 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics Lexan® HFD1830 PC Copolymer (Asia Pacific)
40 MFR LEXAN High Flow Ductile Copolymer UV Stabilized, available in transparent colors only
Impact Test 95.0 J
70.1 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics Lexan® HPF0 PC Copolymer
40 MFR LEXAN High Flow Ductile Copolymer Healthcare Grade
Impact Test 95.0 J
70.1 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics Lexan® HFD1810 PC Copolymer (Europe-Africa-Middle East)
40 MFR LEXAN High Flow Ductile Copolymer
Impact Test 95.0 J
70.1 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics Lexan® HFD1830 PC Copolymer (Europe-Africa-Middle East)
40 MFR LEXAN High Flow Ductile Copolymer UV Stabilized, available in transparent colors only
Impact Test 95.0 J

@Temperature 23.0 °C
70.1 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Xylex X7200 PC+POLYESTER (Asia Pacific)
General purpose, UV stabilised Xylex gradeThis data was supplied by SABIC-IP for the Asia Pacific region.
Impact Test 95.0 J

@Temperature 23.0 °C
70.1 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Xylex X7200 PC+POLYESTER (Europe-Africa-Middle East)
General purpose, UV stabilised Xylex gradeThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Impact Test 95.0 J

@Temperature 23.0 °C
70.1 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Xylex X7200MR PC+POLYESTER (Asia Pacific)
Mold Release version of X7200This data was supplied by SABIC-IP for the Asia Pacific region.
Impact Test 95.0 J

@Temperature 23.0 °C
70.1 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Xylex X7200MR PC+POLYESTER (Europe-Africa-Middle East)
Mold Release version of X7200This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Impact Test 95.0 J

@Temperature 23.0 °C
70.1 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Xylex X7300OQ PC+POLYESTER (Asia Pacific)
PC+ POLYESTER unreinforced alloy developed for optical or lense market. High flow with good impact and excellent optical quality.This data was supplied by SABIC-IP for the Asia Pacific region.
Impact Test 95.0 J

@Temperature 23.0 °C
70.1 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Xylex X7300OQ PC+POLYESTER (Europe-Africa-Middle East)
PC+ POLYESTER unreinforced alloy developed for optical or lense market. High flow with good impact and excellent optical quality.This data was supplied by SABIC-IP for the Europe-Africa-Middle East..
Impact Test 95.0 J

@Temperature 23.0 °C
70.1 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Xylex X8300HP PC+POLYESTER (Asia Pacific)
Transparent, US Food Contact compliant, chemically resistant. This grade will no longer be supported with biocompatibility information and should not be used for medical applications which require b..
Impact Test 95.0 J

@Temperature 23.0 °C
70.1 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Xylex X8300HP PC+POLYESTER (Europe-Africa-Middle East)
Transparent, US Food Contact compliant, chemically resistant. This grade will no longer be supported with biocompatibility information and should not be used for medical applications which require b..
Impact Test 95.0 J
70.1 ft-lb
tempering temperature of 600°C. Specimen size: 7x10x55 mm unnotched. Hardened at 1020°C. Quenched in air. Tempered twice
Assab Steels VANADIS 4 Cold Work Steel
VANADIS 4 is a chromium-molybdenum-vanadium alloyed steel which is characterized by:High wear resistanceHigh compressive strengthVery good through-hardening propertiesVery good toughnessExcellent di..
Impact Test 95.0 J
70.1 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics Lexan® EXRL0672 PC Copolymer
40 MFR LEXAN High Flow Ductile CopolymerThis data was supplied by SABIC-IP for the Americas region.
Impact Test 95.0 J
70.1 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics Lexan® HFD1810 PC Copolymer
40 MFR LEXAN High Flow Ductile Copolymer
Impact Test 95.0 J
70.1 ft-lb
Multiaxial Impact; ISO 6603
SABIC Innovative Plastics Lexan® HFD1810 PC Copolymer (Asia Pacific)
40 MFR LEXAN High Flow Ductile Copolymer