Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 75.9 J @Thickness 3.17 mm, Temperature -40.0 °C |
56.0 ft-lb @Thickness 0.125 in, Temperature -40.0 °F |
ARM impact |
A. Schulman SUPERLINEAR™ XL 0360 Rotational Molding Resin DescriptionSuperlinear XL 0360 is compounded rotational molding resin based on metallocean catalyst technology. This technology allows for high impact and excellent stiffness. It is typically used.. |
|||
Impact Test | 75.9 J @Thickness 3.17 mm, Temperature -40.0 °C |
56.0 ft-lb @Thickness 0.125 in, Temperature -40.0 °F |
ARM impact |
A. Schulman SUPERLINEAR™ XL 0360 Rotational Molding Resin DescriptionSuperlinear XL 0360 is compounded rotational molding resin based on metallocean catalyst technology. This technology allows for high impact and excellent stiffness. It is typically used.. |
|||
Impact Test | 75.9 J @Thickness 3.17 mm, Temperature -40.0 °C |
56.0 ft-lb @Thickness 0.125 in, Temperature -40.0 °F |
ARM impact |
A. Schulman SUPERLINEAR™ XL 0360 Rotational Molding Resin DescriptionSuperlinear XL 0360 is compounded rotational molding resin based on metallocean catalyst technology. This technology allows for high impact and excellent stiffness. It is typically used.. |
|||
Impact Test | 75.9 J @Thickness 3.17 mm, Temperature -40.0 °C |
56.0 ft-lb @Thickness 0.125 in, Temperature -40.0 °F |
ARM impact |
A. Schulman SUPERLINEAR™ XL 0360 Rotational Molding Resin DescriptionSuperlinear XL 0360 is compounded rotational molding resin based on metallocean catalyst technology. This technology allows for high impact and excellent stiffness. It is typically used.. |
|||
Impact Test | 75.9 J @Thickness 3.17 mm, Temperature -40.0 °C |
56.0 ft-lb @Thickness 0.125 in, Temperature -40.0 °F |
ARM impact |
A. Schulman SUPERLINEAR™ XL 0360 Rotational Molding Resin DescriptionSuperlinear XL 0360 is compounded rotational molding resin based on metallocean catalyst technology. This technology allows for high impact and excellent stiffness. It is typically used.. |
|||
Impact Test | 75.9 J @Thickness 3.17 mm, Temperature -40.0 °C |
56.0 ft-lb @Thickness 0.125 in, Temperature -40.0 °F |
ARM impact |
A. Schulman SUPERLINEAR™ XL 0360 Rotational Molding Resin DescriptionSuperlinear XL 0360 is compounded rotational molding resin based on metallocean catalyst technology. This technology allows for high impact and excellent stiffness. It is typically used.. |