Polymer Property : Impact Test = 56.0 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Impact Test 75.9 J

@Thickness 3.17 mm,
Temperature -40.0 °C
56.0 ft-lb

@Thickness 0.125 in,
Temperature -40.0 °F
ARM impact
A. Schulman SUPERLINEAR™ XL 0360 Rotational Molding Resin
DescriptionSuperlinear XL 0360 is compounded rotational molding resin based on metallocean catalyst technology. This technology allows for high impact and excellent stiffness. It is typically used..
Impact Test 75.9 J

@Thickness 3.17 mm,
Temperature -40.0 °C
56.0 ft-lb

@Thickness 0.125 in,
Temperature -40.0 °F
ARM impact
A. Schulman SUPERLINEAR™ XL 0360 Rotational Molding Resin
DescriptionSuperlinear XL 0360 is compounded rotational molding resin based on metallocean catalyst technology. This technology allows for high impact and excellent stiffness. It is typically used..
Impact Test 75.9 J

@Thickness 3.17 mm,
Temperature -40.0 °C
56.0 ft-lb

@Thickness 0.125 in,
Temperature -40.0 °F
ARM impact
A. Schulman SUPERLINEAR™ XL 0360 Rotational Molding Resin
DescriptionSuperlinear XL 0360 is compounded rotational molding resin based on metallocean catalyst technology. This technology allows for high impact and excellent stiffness. It is typically used..
Impact Test 75.9 J

@Thickness 3.17 mm,
Temperature -40.0 °C
56.0 ft-lb

@Thickness 0.125 in,
Temperature -40.0 °F
ARM impact
A. Schulman SUPERLINEAR™ XL 0360 Rotational Molding Resin
DescriptionSuperlinear XL 0360 is compounded rotational molding resin based on metallocean catalyst technology. This technology allows for high impact and excellent stiffness. It is typically used..
Impact Test 75.9 J

@Thickness 3.17 mm,
Temperature -40.0 °C
56.0 ft-lb

@Thickness 0.125 in,
Temperature -40.0 °F
ARM impact
A. Schulman SUPERLINEAR™ XL 0360 Rotational Molding Resin
DescriptionSuperlinear XL 0360 is compounded rotational molding resin based on metallocean catalyst technology. This technology allows for high impact and excellent stiffness. It is typically used..
Impact Test 75.9 J

@Thickness 3.17 mm,
Temperature -40.0 °C
56.0 ft-lb

@Thickness 0.125 in,
Temperature -40.0 °F
ARM impact
A. Schulman SUPERLINEAR™ XL 0360 Rotational Molding Resin
DescriptionSuperlinear XL 0360 is compounded rotational molding resin based on metallocean catalyst technology. This technology allows for high impact and excellent stiffness. It is typically used..