Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 6.91 J | 5.10 ft-lb | High Speed Impact (Energy Max Load); ISO 6603-2 |
Premix Premi-Glas® 1285VE 1285 VE Glass Reinforced Vinyl Ester SMC
(discontinued **) Description: Premi-Glas® 1285 VE is a glass reinforced vinyl ester sheet molding compound designed for automotive under the hood applications. Key features and benefits: Designed for compression mo.. |